SABIC® PC Resin PC1000

SABIC® PC Resin

Sabic PC Resin PC1000 Compounding Grade

Sabic PC1000 is a heat-stabilized, medium-flow polycarbonate designed for custom compounding. It offers excellent mechanical strength, high impact resistance, and good clarity, providing a versatile base for your engineered material solutions.

  • Character: a medium-low flow (MFR = 10 at 300°C/1.2kg), heat stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Stress at Yield: 63 MPa
  • Flexural Modulus: 2300 MPa
  • Izod Impact (Notched): 800 J/m (ASTM)
  • Hardness (Rockwell R): 120
  • Heat Deflection Temp (HDT) @ 1.82 MPa: 127°C
  • Vicat Softening Temperature: 143°C
  • UL94 Flame Rating: V-2 @ 1.6mm
  • Melt Flow Rate (300°C/1.2kg): 10 g/10 min
  • Light Transmission (2.54mm): 88-90%
  • Volume Resistivity: >1E+15 Ω·cm
  • Dielectric Strength: 27 kV/mm
  • Melt Temperature: 280 – 310°C
  • Mold Temperature: 80 – 110°C
  • Drying: 2-4 hours at 120°C

Application

  • Electrical Components
  • Consumer & Industrial Goods
  • Transparent Functional Parts
  • Automotive Interiors
  • Custom Compounded Materials

Features & Benefits

Robust Impact Resistance & Toughness

With its notch-insensitive nature and high impact strength, Sabic PC1000 prevents catastrophic failure from sudden impacts, ideal for durable components and protective housings.

Excellent Thermal Performance & Stability

This heat-stabilized SABIC PC Resin PC1000 maintains integrity at high temperatures, ensuring dimensional stability in demanding environments and during processing.

Superior Clarity & Electrical Properties

It offers high light transmission and low haze for clear applications, alongside strong dielectric strength for safe use in electrical enclosures and insulating components.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top