SABIC® PC Resin PC1003R

SABIC® PC Resin

Sabic PC Resin PC1003R Injection Molding Grade

Sabic PC1003R is a medium-flow, heat and UV-stabilized polycarbonate with built-in mold release. It is a versatile, high-performance plastic designed for reliable general-purpose injection molding, balancing ease of processing with excellent mechanical properties.

  • Character: medium-low flow (MFR = 10 at 300°C/1.2kg), heat and UV stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 63 MPa
  • Flexural Modulus: 2300 MPa
  • Izod Impact, Notched: 800 J/m (ASTM)
  • Rockwell Hardness (R Scale): 120
  • Heat Deflection Temp (HDT) @ 1.82 MPa: 127°C
  • Vicat Softening Temperature: 143°C
  • Melt Flow Rate (300°C/1.2kg): 10 g/10 min
  • Mold Shrinkage: 0.5 – 0.7%
  • Specific Gravity: 1.2
  • UL 94 Flame Rating: V-2 at 1.6 mm
  • Volume Resistivity: >1.5E+15 Ω·cm
  • Dielectric Strength: 27 kV/mm
  • Light Transmission (2.54mm): 88 – 90%
  • Haze: <0.8%

Application

  • Consumer Electronics Housings
  • Automotive Interior Components
  • Electrical Enclosures and Connectors
  • Household Appliances and Tools
  • Various Durable Consumer Goods

Features & Benefits

Superior Impact Resistance & Toughness

With its notch-insensitive nature and high ductility, Sabic PC1003R produces incredibly tough parts that resist cracking and withstand sudden impacts, reducing breakage and product failure in demanding environments.

Excellent Thermal & UV Stability

This resin maintains its structural integrity and appearance under high temperatures and prolonged sun exposure, ensuring long-term performance and color stability for both indoor and outdoor applications.

Enhanced Mold Release & Processability

The built-in mold release agent facilitates easier part ejection and shorter cycle times, boosting your production efficiency and reducing the need for external release agents that can contaminate molds.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top