Sabic PC Resin PC1004R Injection Molding Grade
Sabic PC1004R is a natural, heat-stabilized polycarbonate with mold release. This medium-flow grade is ideal for general-purpose molding and is food contact compliant in most regions, offering a perfect balance of performance and processability.
- Character: medium-low flow (MFR = 10 at 300°C/1.2kg), natural, heat stabilized
Key technical data
- Tensile Stress at Yield: 63 MPa
- Flexural Modulus: 2300 MPa
- Izod Impact, Notched (23°C): 800 J/m (ASTM) | 70 kJ/m² (ISO)
- Heat Deflection Temp (HDT) @ 1.82 MPa: 127 °C
- Vicat Softening Temperature: 143 °C
- Melt Flow Rate (300°C/1.2kg): 10 g/10 min
- Mold Shrinkage: 0.5 – 0.7 %
- Specific Gravity: 1.2
- Recommended Melt Temperature: 280 – 310 °C
- Light Transmission (2.54mm): 88 – 90%
- Haze: <0.8% UL 94 Flame Class Rating: 94V-2 @ 1.6 mm Volume Resistivity: >1.E+15 Ω·cm
Application
- Consumer Goods Housings and Components
- Food Contact Compliant Containers and Utensils
- Electrical Enclosures and Housings
- Light-Diffusing and Translucent Parts
- Various Injection-Molded Industrial and Consumer Parts
Features & Benefits

Related Sabic® Polycarbonate Products
SABIC® PC Resin PC5800
SABIC® PC Resin PC2200R
SABIC® PC Resin PC2203R
SABIC® PC Resin PC2200
SABIC® PC Resin PC1804R
SABIC® PC Resin PC1800R
SABIC® PC Resin PC1803R
SABIC® PC Resin PC1800
SABIC® PC Resin PC1004R
SABIC® PC Resin PC1003R
SABIC® PC Resin PC1000R
SABIC® PC Resin PC1000
SABIC® PC Resin PC0800
SABIC® PC Resin PC0703R
SABIC® PC Resin PC0700
SABIC® PC Resin ALS02
SABIC® PC Resin ALS01
Advanced Manufacturing