Sabic PC Resin PC1800 General Purpose Grade
Sabic PC1800 is a medium-high flow, heat-stabilized polycarbonate. It’s engineered for custom compounding, offering excellent processability and robust mechanical properties for demanding industrial applications.
- Character: medium-high flow (MFR = 10 at 300°C/1.2kg), heat stabilized
Key technical data
- Tensile Strength at Yield: 63 MPa
- Flexural Modulus: 2300 MPa
- Notched Izod Impact (23°C): 700 J/m (ASTM)
- Heat Deflection Temp (HDT) @ 1.82 MPa: 124 °C
- Vicat Softening Temperature: 141 °C
- Melt Flow Rate (300°C/1.2kg): 18 g/10 min
- Specific Gravity: 1.20
- UL 94 Flame Rating: V-2 @ 1.6mm
- Volume Resistivity: >1E+15 Ω·cm
- Melt Temperature: 280 – 300 °C
- Mold Temperature: 80 – 100 °C
- Drying: 2-4 hours at 120°C
Application
- Custom Compounded Materials
- Electrical Enclosures and Housings
- Automotive Interior Components
- Consumer Electronics Parts
- Industrial Machine Components
- Connectors and Electrical Components
Features & Benefits

Related Sabic® Polycarbonate Products
SABIC® PC Resin PC5800
SABIC® PC Resin PC2200R
SABIC® PC Resin PC2203R
SABIC® PC Resin PC2200
SABIC® PC Resin PC1804R
SABIC® PC Resin PC1800R
SABIC® PC Resin PC1803R
SABIC® PC Resin PC1800
SABIC® PC Resin PC1004R
SABIC® PC Resin PC1003R
SABIC® PC Resin PC1000R
SABIC® PC Resin PC1000
SABIC® PC Resin PC0800
SABIC® PC Resin PC0703R
SABIC® PC Resin PC0700
SABIC® PC Resin ALS02
SABIC® PC Resin ALS01
Advanced Manufacturing