Sabic PC Resin PC1800R General Purpose Grade

Sabic PC1800R is a medium-high flow, heat-stabilized polycarbonate with an internal mold release. It is engineered for high-performance, efficiency, and reliability in general-purpose injection molding applications.

  • Character: a medium-high flow (MFR = 18 at 300°C/1.2kg), heat stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Tensile Stress at Yield: 63 MPa
  • Flexural Modulus: 2300 MPa
  • Notched Izod Impact (23°C): 700 J/m (ASTM)
  • Heat Deflection Temp (HDT) @ 1.82 MPa: 124°C
  • Vicat Softening Temperature: 141°C
  • Physical & Processing Properties
  • Melt Flow Rate (300°C/1.2kg): 18 g/10 min
  • Mold Shrinkage: 0.5 – 0.7%
  • Specific Gravity: 1.2
  • Volume Resistivity: >1.E+15 Ω·cm
  • Dielectric Strength: 27 kV/mm
  • UL 94 Flame Rating: V-2 at 1.6mm
  • Optical Properties (For transparent applications)
  • Light Transmission (2.54mm): 88 – 90%
  • Haze: <0.8%

Application

  • Consumer Electronics Housings & Components
  • Automotive Interior Parts
  • Electrical Enclosures and Connectors
  • Appliances and Tool Housings
  • Various Durable Consumer and Industrial Goods

Features & Benefits

Excellent Flow

With a medium-high melt flow rate, Sabic PC1800R fills intricate molds effortlessly, reducing short shots and enabling the production of complex, thin-walled parts with high detail and superior surface finish.

Outstanding Impact Resistance & Toughness

This grade delivers exceptional notched Izod impact strength, ensuring your products can withstand accidental drops, impacts, and rough handling without cracking, leading to greater durability and customer satisfaction.

High Heat Resistance & Stability

Featuring a Heat Deflection Temperature of 124°C at 1.82 MPa, components made from SABIC PC1800R maintain their structural integrity in elevated temperature environments, ensuring reliable performance and safety.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top