Sabic PC Resin PC2200R Injection Molding Grade
Sabic PC2200R is a high-flow, heat-stabilized polycarbonate with built-in mold release. It simplifies production for high-volume, general-purpose molding, delivering excellent performance and faster cycle times.
- Character: high flow (MFR = 22 at 300°C/1.2kg), heat stabilized
Key technical data
- Melt Flow Rate (300°C/1.2kg): 22 g/10 min
- Tensile Strength at Yield: 63 MPa
- Notched Izod Impact (23°C): 640 J/m (ASTM)
- Heat Deflection Temp (1.82 MPa): 122 °C
- Light Transmission (2.54mm): 88-90%
- Flame Rating: UL 94 V-2 @ 1.6mm
- Flexural Modulus: 2300 MPa
- Specific Gravity: 1.20
Application
- Consumer Electronics Housings
- Automotive Interior Components
- Electrical Enclosures and Connectors
- Industrial Parts and Housings
- Various Durable Consumer Goods
Features & Benefits

Related Sabic® Polycarbonate Products
SABIC® PC Resin PC5800
SABIC® PC Resin PC2200R
SABIC® PC Resin PC2203R
SABIC® PC Resin PC2200
SABIC® PC Resin PC1804R
SABIC® PC Resin PC1800R
SABIC® PC Resin PC1803R
SABIC® PC Resin PC1800
SABIC® PC Resin PC1004R
SABIC® PC Resin PC1003R
SABIC® PC Resin PC1000R
SABIC® PC Resin PC1000
SABIC® PC Resin PC0800
SABIC® PC Resin PC0703R
SABIC® PC Resin PC0700
SABIC® PC Resin ALS02
SABIC® PC Resin ALS01
Advanced Manufacturing