Kibisan® PN-107 L125 General Purpose Grade SAN Resin
Kibisan PN-107 L125 SAN Resin is a high-flow, crystal-clear plastic perfect for food containers, sealed cans, and cosmetic boxes. Its smooth flow speeds up production, saving time and costs, while the glass-like transparency lets products shine on shelves. Lightweight yet tough, it resists cracks, heat (up to 90°C), and yellowing—ideal for FDA-compliant packaging that needs to look good and last.
- Manufacturer: CHIMEI
- Character: High flowability, high transparency
- Application: Food containers, sealed cans, cosmetic boxes

Download
Access essential product documentation including technical datasheets, safety information, environmental certifications, and processing guides. All documents are sourced directly from manufacturers and updated regularly for accuracy.

Kibisan® PN-107 L125 Datasheet
| General SAN KIBISAN® PN-107 L125 | ||||
| Product Description: High clarity | ||||
| Properties | ISO Test Method | Test Condition | Unit | PN-107_L125 |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 58 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.06 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 65 |
| 50 mm/min, break | MPa | 65 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 3 |
| Flexural Strength | 178 | 2 mm/min | MPa | 89 |
| Flexural Modulus | 178 | 2 mm/min | GPa | 2.6 |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 2 |
| -30℃, Notched | KJ/m2 | – | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 2 |
| -30℃, Notched | KJ/m2 | – | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 104 |
| 50℃/hr;5KG | ℃ | 101 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 88 |
| 1.8MPa, annealed | ℃ | 99 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 3.6~3.8*10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB |
| Mold Shrinkage | 294-4 | – | % | 0.2~0.7 |
| Symbol | 1043 | – | – | >SAN< |
| March 11, 2024 | ||||
Kibisan® PN-107 L125 UL Product iQ
| KIBISAN® PN-107(+) UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Styrene Acrylonitrile (SAN) “KIBISAN”, furnished as pellets |
| (+) – Indicate 0~0.5% acid scavengers. | ||
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 5 | |
| 3.0 mm | PLC 4 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 1 | |
| 3.0 mm | PLC 1 | |
| Comparative Tracking Index (CTI) | PLC 2 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 1 | |
| High Voltage, Low Current Arc Resistance | PLC 6 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
Related Kibisan® SAN (aS) Plastics
Chimei Kibisan® PN-137H SAN
Chimei Kibisan® PN-127 L150FG
Chimei Kibisan® PN-127 L200
Chimei Kibisan® PN-127 L150
Chimei Kibisan® PN-117H L150FG
Chimei Kibisan® PN-117C
Chimei Kibisan® PN-117 L100
Chimei Kibisan® PN-106 L150
Chimei Kibisan® PN-127H SAN
Chimei Kibisan® PN-107 L125 SAN
Chimei Kibisan® PN-117 L200 SAN
Chimei Kibisan® PN-127 L100
Chimei Kibisan® PN-107 L125FG
Advanced Manufacturing