Chimei Kibisan® PN-117 L200 SAN

Chimei Kibisan PN-117 L200 SAN Resin

Kibisan® PN-117 L200 Injection Molding General SAN Resin

The Kibisan PN-117 L200 is a vibrant transparent blue SAN resin designed for clarity and visual appeal. Its sleek, semi-transparent finish makes it perfect for products where aesthetics matter. Available in easy-to-melt pellets, this material flows smoothly into molds, even for intricate designs. Whether you’re crafting colorful cosmetic jars or eye-catching homeware, the PN-117 L200 delivers consistent color and gloss.

  • Manufacturer: CHIMEI
  • Application: General injection molding for daily commodities, transparent family hardware products, cosmetic containers
  • Character: Transparent blue
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Vibrant Transparent Blue Finish

The Kibisan PN-117 L200 offers a striking transparent blue hue, ideal for eye-catching cosmetic containers or decorative household items. Its clarity enhances product aesthetics without extra coatings.

Fast-Flowing for Detailed Molding

With a 32 ml/10min melt flow rate, this SAN resin fills molds quickly, reducing cycle times for high-volume production of intricate designs like thin-walled jars or hardware parts.

Durable & Heat-Resistant Performance

Boasting 68 MPa tensile strength and 104°C Vicat softening, chimei PN-117 L200 withstands daily wear, hot water, and repeated use—perfect for dishwasher-safe items or sturdy storage solutions.

Kibisan PN-117 L200 SAN Resin

Download

Access essential product documentation including technical datasheets, safety information, environmental certifications, and processing guides. All documents are sourced directly from manufacturers and updated regularly for accuracy.

Chimei Kibisan® PN-117 L200 Application

Kibisan® PN-117 L200 Datasheet

General SAN KIBISAN® PN-117 L200
Product Description: Injection molding
PropertiesISO Test MethodTest ConditionUnitPN-117_L200
Melt Flow Index1133220℃×10KGml/10 min32
Mass Density118323  ℃g/cm31.06
Tensile Strength52750 mm/min, yieldMPa68
50 mm/min, breakMPa68
Tensile Elongation52750 mm/min%3
Flexural Strength1782 mm/minMPa93
Flexural Modulus1782 mm/minGPa3
Izod Impact Strength180/1A23℃, NotchedKJ/m22
-30℃, NotchedKJ/m2
Charpy Impact Strength17923℃, NotchedKJ/m22
-30℃, NotchedKJ/m2
Vicat Softening Temp.30650℃/hr;1KG104
50℃/hr;5KG102
Heat Distortion Temp.75/A1.8MPa, unannealed89
1.8MPa, annealed100
Coefficient of Linear Thermal Expansion113593.6~3.8*10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.2~0.7
Symbol1043>SAN<
March 11, 2024

Kibisan® PN-117 L200 UL Product iQ

KIBISAN® PN-117 UL Product iQ
File Number: E56070Yellow Card™Styrene Acrylonitrile (SAN) “KIBISAN”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)PLC 4UL 746A
(1.5 mm)
High Amp Arc Ignition (HAI)PLC 0UL 746A
(1.5 mm)
High Voltage Arc Tracking Rate (HVTR)PLC 0
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top