Chimei Kibisan® PN-127 L200 General Transparent Dark Blue
Chimei KIBISAN PN-127 L200 is a high-performance SAN resin designed for injection molding. This General SAN plastic stands out with its transparent dark blue color and heat-resistant properties, making it a versatile choice for industries needing both clarity and durability. Whether you’re crafting visually appealing products or parts that must withstand high temperatures, this resin delivers reliability and quality.
- Application: External pen tubing/transparent parts for electrical and electronic products/fan blades
- Character: Transparent dark blue, Heat Resistant Grade
Key technical data (ISO)
- Melt Flow Index: 17 ml/10 min
- Mass Density: 1.06 g/cm³
- Tensile Strength: 74 MPa (yield and break)
- Flexural Strength: 105 MPa
- Impact Strength: Izod 3 kJ/m², Charpy 2 kJ/m² (notched)
- Vicat Softening Temperature: 105°C (1 kg), 104°C (5 kg)
- Heat Distortion Temperature: 90°C (unannealed), 101°C (annealed)
- Flammability: HB under UL-94 at 1.5 mm thickness
- Mold Shrinkage: 0.2~0.7%

Applications
- External Pen Tubing: Its transparency and blue tint enhance visual appeal, while heat resistance ensures durability during daily use, solving issues of aesthetic and functional wear.
- Transparent Parts for Electrical and Electronic Products: Combines clarity for visibility with electrical insulation, addressing needs for safe, see-through components in devices.
- Fan Blades: Offers mechanical strength and heat resistance, suitable for smaller fans, tackling challenges of durability in warmer operating conditions.

Kibisan® PN-127 L200 Datasheet
| General SAN KIBISAN® PN-127_L200 Product Description: Injection molding | ||||
| Properties | ISO Test Method | Test Condition | Unit | PN-127_L200 |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 17 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.06 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 74 |
| 50 mm/min, break | MPa | 74 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 3 |
| Flexural Strength | 178 | 2 mm/min | MPa | 105 |
| Flexural Modulus | 2 mm/min | GPa | 3.3 | |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 3 |
| -30℃, Notched | KJ/m2 | – | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 2 |
| -30℃, Notched | KJ/m2 | – | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 105 |
| 50℃/hr;5KG | ℃ | 104 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 90 |
| 1.8MPa, annealed | ℃ | 101 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 3.6~3.8*10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB |
| Mold Shrinkage | 294-4 | – | % | 0.2~0.7 |
| Symbol | 1043 | – | – | >SAN< |
| March 11, 2024 Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test | ||||
Kibisan® PN-127 L200 UL Product iQ
| KIBISAN® PN-127 | UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets |
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | PLC 4 | UL 746A |
| (1.5 mm) | ||
| High Amp Arc Ignition (HAI) | PLC 0 | UL 746A |
| (1.5 mm) | ||
| High Voltage Arc Tracking Rate (HVTR) | PLC 0 | |
| High Voltage, Low Current Arc Resistance | PLC 6 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
Related Kibisan® SAN (aS) Plastics
Chimei Kibisan® PN-137H SAN
Chimei Kibisan® PN-127 L150FG
Chimei Kibisan® PN-127 L200
Chimei Kibisan® PN-127 L150
Chimei Kibisan® PN-117H L150FG
Chimei Kibisan® PN-117C
Chimei Kibisan® PN-117 L100
Chimei Kibisan® PN-106 L150
Chimei Kibisan® PN-127H SAN
Chimei Kibisan® PN-107 L125 SAN
Chimei Kibisan® PN-117 L200 SAN
Chimei Kibisan® PN-127 L100
Chimei Kibisan® PN-107 L125FG
Advanced Manufacturing