Chimei WONDERLITE® PC-110P

Chimei WONDERLITE PC-108U PC Resin

WONDERLITE PC-110P Medical Grade PC Material

Chimei Wonderlite PC-110P is a medical-grade polycarbonate resin engineered for safety and durability. Compliant with ISO10993-5/10 bio-compatibility standards, it combines medium viscosity with exceptional impact resistance and thermal stability. Ideal for pharmacological packaging and medical devices, it ensures reliability in critical healthcare applications.

  • Character: Comply with Bio-compatibility test (ISO10993-5/10)
  • Application: Medical application
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 10 ml/10 min (300°C)
  • Tensile Strength: 65 MPa (yield)
  • Heat Distortion Temp.: Up to 143°C (annealed)
  • Flammability: UL-94 V-2 (2.5mm)
  • Mold Shrinkage: 0.5–0.7%

Unmatched Impact Resistance

With an Izod Impact Strength of 75 KJ/m² (23°C, notched), Medical Grade PC-110P withstands drops, shocks, and repeated stress. Perfect for surgical tools or protective housings that demand rugged performance.

High-Temperature Stability

Boasting a Vicat Softening Temperature of 150°C (1KG load), this material retains structural integrity during sterilization (e.g., autoclaving) or exposure to hot environments, ensuring longevity in medical workflows.

Regulatory Compliance & Safety

Pharmacological Package PC WONDERLITE® PC-110P meets FDA standards and UL-94 V-2 flammability ratings, making it safe for drug containers, IV components, and other applications requiring strict hygiene and fire resistance.

WONDERLITE® PC-110P

Application

  • Surgical Instrument Trays: Withstands repeated sterilization without cracking.
  • Pharmacological Packaging: Safe for drug storage, resistant to chemical interactions.
  • Medical Imaging Components: Maintains clarity and strength in MRI/CT machine parts.
Chimei Wonderlite PC-110P Application

WONDERLITE® PC-110P Datasheet

Pharmacological Package PC WONDERLITE®  PC-110P
Product Description: Medium viscosity
PropertiesISO Test MethodTest ConditionUnitPC-110P
Melt Flow Index1133 300℃×1.2KGml/10 min10 
Mass Density1183 23 ℃g/cm31.2 
Tensile Strength527 50 mm/min, yieldMPa65 
50 mm/min, breakMPa75 
Tensile Elongation527 50 mm/min%120 
Flexural Strength178 2 mm/minMPa90 
Flexural Modulus2 mm/minGPa2.4 
Izod Impact Strength180/1A23℃, Notched,1/8″KJ/m275 
-30℃, Notched,1/8″KJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m275 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG150 
50℃/hr;5KG145 
Heat Distortion Temp.75/A1.8MPa, unannealed128 
1.8MPa, annealed143 
Coefficient of Linear Thermal Expansion11359 6.0~8.0×10-5
FlammabilityUL-942.5mm V-2
Mold Shrinkage294-4%0.5~0.7
Symbol1043 >PC<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top