Chimei WONDERLITE® PC-110u

Chimei-WONDERLITE-PC-110U

WONDERLITE® PC-110u Weather Resistant Grade UV Resistant Medium viscosity

WONDERLITE PC-110U is a premium UV-stabilized polycarbonate resin designed for outdoor applications. This versatile PC-110u grade offers excellent weather resistance and optical clarity, making it perfect for traffic signs and other exterior uses.This medium-viscosity resin delivers reliable performance and durability in challenging environments.

  • Application: Outdoor applications, traffic signs
  • Character: Transparent grade, Weather Resistant grade, UV resistant, medium viscosity
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.

Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=
Chimei WONDERLITE® PC-110U Application

Superior UV and Weather Protection

Our PC-110u features advanced UV stabilizers that effectively shield against sunlight degradation, ensuring your outdoor applications maintain durability and clarity over time.

Exceptional Mechanical Strength and Stability

Wonderlite PC-110u offers impressive tensile strength (65 MPa) and flexural strength (90 MPa), providing reliable performance in demanding outdoor environments.

Easy Processing and Versatile Applications

With its medium viscosity and stable processing characteristics, CHIMEI PC-110u polycarbonate resin ensures smooth production while maintaining excellent surface quality.

WONDERLITE® PC-110U

WONDERLITE® PC-110u Datasheet

UV Stabilized PC WONDERLITE® PC-110U
Product Description: UV Stabilized
PropertiesISO Test MethodTest ConditionUnitPC-110U
Melt Flow Index1133300℃ × 1.2KGml/10 min10
Mass Density118323  ℃g/cm31.2
Tensile Strength52750 mm/min, yieldMPa65
50 mm/min, breakMPa75
Tensile Elongation52750 mm/min%120
Flexural Strength1782 mm/minMPa90
Flexural Modulus1782 mm/minGPa2.4
Izod Impact Strength180/1A23℃, Notched,1/8″KJ/m275
-30℃, Notched,1/8″KJ/m2
Charpy Impact Strength17923℃, NotchedKJ/m275
-30℃, NotchedKJ/m2
Vicat Softening Temp.30650℃/hr;1KG148
50℃/hr;5KG143
Heat Distortion Temp.75/A1.8MPa, unannealed127
1.8MPa, annealed142
Coefficient of Linear Thermal Expansion113596.0~8.0×10-5
FlammabilityUL-941.5mm V-2
Mold Shrinkage294-4%0.5~0.7
Symbol1043>PC<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test

WONDERLITE® PC-110U (f1)(a) UL Product iQ

WONDERLITE® PC-110U(f1)(a) | UL Product iQ
File Number: E56070Yellow Card™Polycarbonate (PC) “WONDERLITE”, furnished as pellets
(f1) – Suitable for outdoor use with respect to exposure to Ultraviolet Light, Water Exposure and Immersion in accordance with UL 746C.
(a) – Ball pressure temperature is in accordance with IEC 60695-10-2 Method B.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
0.75 mm, Color: ALLV-2
1.5 to 1.7 mm, Color: ALLV-2
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
0.75 mm, Color: ALLV-2
1.5 to 1.7 mm, Color: ALLV-2
3.0 mm, Color: ALLHB40
Glow Wire Ignition Temperature (GWIT)IEC 60695-2-13
1.5 to 1.7 mm850   °C
3.0 mm875   °C
Glow Wire Flammability Index (GWFI)IEC 60695-2-12
1.5 to 1.7 mm850   °C
3.0 mm960   °C
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
0.75 mmPLC 4
1.5 to 1.7 mmPLC 4
3.0 mmPLC 2
High Amp Arc Ignition (HAI)UL 746A
0.75 mmPLC 4
1.5 to 1.7 mmPLC 4
3.0 mmPLC 3
Comparative Tracking Index (CTI)PLC 2UL 746A
Dielectric Strength30   kV/mmASTM D149
High Voltage Arc Tracking Rate (HVTR)PLC 2
Volume Resistivity1.0E+14   ohms·cmASTM D257/IEC 60093
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
0.75 mm125   °C
1.5 to 1.7 mm125   °C
3.0 mm125   °C
Relative Thermal Index – Mechanical ImpactUL 746B
0.75 mm105   °C
1.5 to 1.7 mm105   °C
3.0 mm105   °C
Relative Thermal Index – Mechanical StrengthUL 746B
0.75 mm125   °C
1.5 to 1.7 mm125   °C
3.0 mm125   °C
Ball Pressure Temperature135   °C
PHYSICAL PROPERTIESVALUETEST METHOD
Dimensional Change0.0   %ASTM D1042/ISO 2796
UV Exposure & Water Immersionf1UL 746C
Report Date: 2001-09-25

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top