WONDERLITE® PC-115p Plactic Resin Medical Grade Gamma Resistance Material
Wonderlite PC-115P is a high-quality polycarbonate resin made by CHIMEI. This medical-grade material comes in natural color and is packaged in a 25kg moisture-proof aluminum foil bag for easy storage. With features like high impact strength and UL-94 V-2 flammability rating, it is ideal for medical applications.
- Application: Medical application
- Character: Medical grade
Download
Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.


WONDERLITE® PC-115p Datasheet
| Pharmacological Package PC WONDERLITE® PC-115P | ||||
| Product Description: Low viscosity | ||||
| Properties | ISO Test Method | Test Condition | Unit | PC-115P |
| Melt Flow Index | 1133 | 300℃ × 1.2KG | ml/10 min | 15 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.2 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 65 |
| 50 mm/min, break | MPa | 70 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 120 |
| Flexural Strength | 178 | 2 mm/min | MPa | 90 |
| Flexural Modulus | 178 | 2 mm/min | GPa | 2.4 |
| Izod Impact Strength | 180/1A | 23℃, Notched,1/8″ | KJ/m2 | 70 |
| -30℃, Notched,1/8″ | KJ/m2 | – | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 70 |
| -30℃, Notched | KJ/m2 | – | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 150 |
| 50℃/hr;5KG | ℃ | 145 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 128 |
| 1.8MPa, annealed | ℃ | 143 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 6.0~8.0×10-5 |
| Flammability | – | UL-94 | – | 2.5mm V-2 |
| Mold Shrinkage | 294-4 | – | % | 0.5~0.8 |
| Symbol | 1043 | – | – | >PC< |
| March 11, 2024 | ||||
WONDERLITE® PC-115p UL Product iQ
| WONDERLITE® PC-115P(+) UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Polycarbonate (PC) “WONDERLITE”, furnished as pellets |
| (+) – Indicate 0~0.5% acid scavengers. | ||
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 0.4 mm, Color: ALL | V-2 | |
| 1.5 mm, Color: ALL | V-2 | |
| 2.5 to 2.8 mm, Color: ALL | V-2 | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 0.4 mm, Color: ALL | V-2 | |
| 1.5 mm, Color: ALL | V-2 | |
| 2.5 to 2.8 mm, Color: ALL | V-2 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 0.4 mm | PLC 4 | |
| 1.5 mm | PLC 2 | |
| 2.5 to 2.8 mm | PLC 2 | |
| 3.0 mm | PLC 2 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 0.4 mm | PLC 4 | |
| 1.5 mm | PLC 4 | |
| 2.5 to 2.8 mm | PLC 3 | |
| 3.0 mm | PLC 3 | |
| Comparative Tracking Index (CTI) | PLC 2 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 2 | |
| High Voltage, Low Current Arc Resistance | PLC 6 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 0.4 mm | 80 °C | |
| 1.5 mm | 120 °C | |
| 2.5 to 2.8 mm | 120 °C | |
| 3.0 mm | 120 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 0.4 mm | 80 °C | |
| 1.5 mm | 105 °C | |
| 2.5 to 2.8 mm | 105 °C | |
| 3.0 mm | 105 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 0.4 mm | 80 °C | |
| 1.5 mm | 120 °C | |
| 2.5 to 2.8 mm | 120 °C | |
| 3.0 mm | 120 °C | |
| Report Date: 2001-09-25 | ||
Related WONDERLITE® PC Plastics
Chimei WONDERLITE® PC-6715NF
Chimei WONDERLITE® PC-6710NF
Chimei WONDERLITE® PC-6700
Chimei WONDERLITE® PC-6715VT
Chimei WONDERLITE® PC-6600 J01
Chimei WONDERLITE® PC-681U
Chimei WONDERLITE® PC-616LS
Chimei WONDERLITE® PC-175
Chimei WONDERLITE® PC-145K
Chimei WONDERLITE® PC-122P
Chimei WONDERLITE® PC-115U
Chimei WONDERLITE® PC-115
Chimei WONDERLITE® PC-115L
Chimei WONDERLITE® PC-110P
Chimei WONDERLITE® PC-110L
Chimei WONDERLITE® PC-108U
Chimei WONDERLITE® PC-6610
Chimei WONDERLITE® PC-6710
Chimei WONDERLITE® PC-6600
Chimei WONDERLITE® PC-122u
Chimei WONDERLITE® PC-122
Chimei WONDERLITE® PC-115p
Chimei WONDERLITE® PC-110u
Chimei WONDERLITE® PC-110
Advanced Manufacturing