Chimei WONDERLITE® PC-115U

Chimei Wonderlite PC-115U PC Resin

WONDERLITE PC-115U Weathering Grade Low Viscosity

WONDERLITE PC-115U is a UV-stabilized polycarbonate resin with low viscosity, ideal for durable outdoor applications. It offers easy processing, long-lasting durability, and superior impact resistance, making it suitable for traffic signs and more. It meets high standards for safety and performance, with UL certification for various properties.

  • Application: Outdoor applications, traffic signs
  • Character: Low viscosity, UV stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 15 ml/10 min
  • Density: 1.2 g/cm³
  • Tensile strength: 64 MPa (yield)
  • Tensile elongation: 120%
  • Impact Resistance: High Izod impact strength 70 KJ/m²
  • Thermal Stability: Vicat softening temperature 148 ℃ and heat distortion temperature 127 ℃ (unannealed)
  • Flammability: Rated V-2 for 1.5mm thickness

Easy to Process

PC-115U has a low viscosity, ensuring smooth manufacturing processes like injection molding and extrusion. This can save time and resources, leading to higher quality parts.

Long-Lasting Durabilit

Its UV stabilization means it maintains appearance and performance under sunlight, ideal for outdoor use where materials face constant environmental exposure.

Superior Impact Resistance

With a high Izod impact strength of 70 KJ/m², it’s robust and reliable, perfect for applications needing safety and longevity, like traffic signs.

Wonderlite® PC-115U

Application

  • Traffic Signs
  • Outdoor Advertising Boards
  • Garden and Park Furnishings
  • Roofing Materials
Chimei Wonderlite PC-115U Application

WONDERLITE® PC-115U Datasheet

UV Stabilized PC WONDERLITE®  PC-115U
Product Description: Low viscosity
PropertiesISO Test MethodTest ConditionUnitPC-115U
Melt Flow Index1133 300℃  ×  1.2KGml/10 min15 
Mass Density1183 23 ℃g/cm31.2 
Tensile Strength527 50 mm/min, yieldMPa64 
50 mm/min, breakMPa70 
Tensile Elongation527 50 mm/min%120 
Flexural Strength178 2 mm/minMPa90 
Flexural Modulus2 mm/minGPa2.4 
Izod Impact Strength180/1A23℃, Notched,1/8″KJ/m270 
-30℃, Notched,1/8″KJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m270 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG148 
50℃/hr;5KG143 
Heat Distortion Temp.75/A1.8MPa, unannealed127 
1.8MPa, annealed142 
Coefficient of Linear Thermal Expansion11359 6.0~8.0×10-5
FlammabilityUL-941.5mm V-2
Mold Shrinkage294-4%0.5~0.7
Symbol1043 >PC<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users
should confirm results by their own test.

WONDERLITE® PC-115U UL Product iQ

WONDERLITE® PC-115(+) | UL Product iQ
File Number: E56070Yellow Card™Polycarbonate (PC) “WONDERLITE”, furnished as pellets
(f1) – Suitable for outdoor use with respect to exposure to Ultraviolet Light, Water Exposure and Immersion in accordance with UL 746C
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
0.75 mm, Color: ALLV-2
1.5 to 1.7 mm, Color: ALLV-2
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
0.75 mm, Color: ALLV-2
1.5 to 1.7 mm, Color: ALLV-2
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
0.75 mmPLC 4
1.5 to 1.7 mmPLC 2
3.0 mmPLC 2
High Amp Arc Ignition (HAI)UL 746A
0.75 mmPLC 4
1.5 to 1.7 mmPLC 4
3.0 mmPLC 3
Comparative Tracking Index (CTI)PLC 2UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 2
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
0.75 mm120   °C
1.5 to 1.7 mm120   °C
3.0 mm120   °C
Relative Thermal Index – Mechanical ImpactUL 746B
0.75 mm105   °C
1.5 to 1.7 mm105   °C
3.0 mm105   °C
Relative Thermal Index – Mechanical StrengthUL 746B
0.75 mm120   °C
1.5 to 1.7 mm120   °C
3.0 mm120   °C
PHYSICAL PROPERTIESVALUETEST METHOD
UV Exposure & Water Immersionf1UL 746C

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top