Chimei WONDERLITE® PC-122

Chimei-WONDERLITE-PC-122

WONDERLITE® PC-122 Plastic Resin General Grade Material

Wonderlite PC-122 by CHIMEI is a high-flow polycarbonate resin in granular form, packed in 25kg bags. It’s great for injection molding thin-walled and complex products like pens, toys, and containers. With strong durability, heat resistance up to 150°C, and versatility, it’s perfect for everyday applications.

  • Application: General injection molding for external pen tubing, stationery, toys, water containers, thin wall products, complex transparent molding products
  • Character: High flow grade
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.

Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=
Chimei WONDERLITE® PC-122 Application

High Flow and Easy Molding

Wonderlite PC-122 offers excellent flow properties, making it ideal for injection molding complex designs with smooth, efficient production performance.

Durable and Heat Resistant

This resin boasts strong tensile and flexural strength, maintaining stability under heat up to 150°C for reliable, long-lasting applications.

Versatile for Everyday Applications

Perfect for various uses, Wonderlite PC-122 is used in pens, toys, water containers, and clear, thin-walled, molded products.

WONDERLITE® PC-122

WONDERLITE® PC-122 Datasheet

General PC WONDERLITE® PC-122
Product Description: High flow
PropertiesISO Test MethodTest ConditionUnitPC-122
Melt Flow Index1133300℃ × 1.2KGml/10 min22
Mass Density118323  ℃g/cm31.2
Tensile Strength52750 mm/min, yieldMPa63
50 mm/min, breakMPa70
Tensile Elongation52750 mm/min%120
Flexural Strength1782 mm/minMPa90
Flexural Modulus1782 mm/minGPa2.4
Izod Impact Strength180/1A23℃, Notched,1/8″KJ/m260
-30℃, Notched,1/8″KJ/m2
Charpy Impact Strength17923℃, NotchedKJ/m260
-30℃, NotchedKJ/m2
Vicat Softening Temp.30650℃/hr;1KG150
50℃/hr;5KG145
Heat Distortion Temp.75/A1.8MPa, unannealed128
1.8MPa, annealed143
Coefficient of Linear Thermal Expansion113596.0~8.0×10-5
FlammabilityUL-943.0mm V-2
Mold Shrinkage294-4%0.5~0.7
Symbol1043>PC<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

WONDERLITE® PC-122 UL Product iQ

WONDERLITE® PC-122 UL Product iQ
File Number: E56070Yellow Card™Polycarbonate (PC) “WONDERLITE”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
0.38 mm, Color: ALLV-2
1.6 mm, Color: ALLV-2
3.2 mm, Color: ALLV-2
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
0.38 mm, Color: ALLV-2
1.6 mm, Color: ALLV-2
3.2 mm, Color: ALLV-2
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.6 mmPLC 2
3.2 mmPLC 2
High Amp Arc Ignition (HAI)UL 746A
1.6 mmPLC 0
3.2 mmPLC 0
Comparative Tracking Index (CTI)PLC 3UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 2
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
0.38 mm80   °C
1.6 mm120   °C
3.2 mm120   °C
Relative Thermal Index – Mechanical ImpactUL 746B
0.38 mm80   °C
1.6 mm105   °C
3.2 mm105   °C
Relative Thermal Index – Mechanical StrengthUL 746B
0.38 mm80   °C
1.6 mm120   °C
3.2 mm120   °C
Report Date: 2001-09-25

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top