Chimei WONDERLITE® PC-6600 J01

Chimei Wonderlite PC-6600 J01 PC Resin

Chimei WONDERLITE PC-6600 J01 Standard Black Color

CHIMEI WONDERLITE PC-6600 J01 is a non-brominated, non-chlorinated flame-retardant polycarbonate resin designed for safety-critical applications. Pre-colored in standard black, it achieves UL 94 V-0 certification at just 1.0mm thickness, making it ideal for electrical components, automotive parts, and industrial housings where durability, fire safety, and regulatory compliance are paramount.

  • Application: Electrical appliances
  • Character: Flame retardant (non-brominated, and non-chlorinated), 1.0mm V0, standard black and pre-colored
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flame Retardancy: UL 94 V-0 (1.0mm), 5VA (3.0mm); IEC 60695-11-10/20 certified.
  • Impact Strength: 60 KJ/m² (23°C, notched Izod/Charpy); 15 KJ/m² (-30°C).
  • Vicat Softening Temp: 150°C (1.0mm).
  • Heat Distortion Temp: 140°C (annealed).
  • Glow Wire Ignition (GWIT): 875°C (3.0mm).
  • Dielectric Strength: 31 kV/mm.
  • Volume Resistivity: 1.0E+14 Ω·cm.
  • CTI: PLC 2 (comparative tracking index).
  • Density: 1.2 g/cm³.
  • Mold Shrinkage: 0.4–0.6%.

Halogen-Free Flame Retardancy

WONDERLITE® PC-6600 J01 eliminates toxic bromine/chlorine additives while delivering UL 94 V-0 (1.0mm) and 5VA (3.0mm) flammability ratings. Perfect for electronics and appliances requiring stringent safety compliance without environmental trade-offs.

Extreme Impact Resistance

With 60 KJ/m² Izod impact strength at 23°C, this material withstands drops, vibrations, and harsh environments. Even at -30°C, it retains 15 KJ/m² toughness, ensuring reliability in automotive or outdoor equipment.

High-Temperature Resilience

A Vicat softening temperature of 150°C and heat distortion temperature up to 140°C (annealed) ensure stability in high-heat scenarios like power distribution systems or LED housings.

Wonderlite® PC-6600 J01

Application

  • Circuit breakers & switchgear
  • Power distribution housings
  • LED lighting components
  • Automotive connectors
  • Consumer electronics
Chimei Wonderlite PC-6600 J01 Application

WONDERLITE® PC-6600 J01 Datasheet

Flame Retardant WONDERLITE®  PC-6600 J01
Product Description: 1.0mm V-0, Opaque, Black
PropertiesISO Test MethodTest ConditionUnitPC-
6600_J01
Melt Flow Index1133 300℃  ×  1.2KGml/10 min10 
Spiral flowCHIMEI260℃,2mm,
V:50%,P:50%
cm
Mass Density1183 23 ℃g/cm31.2 
Tensile Strength527 50 mm/min, yieldMPa60 
50 mm/min, breakMPa70 
Tensile Elongation527 50 mm/min%115 
Flexural Strength178 2 mm/minMPa90 
Flexural Modulus2 mm/minGPa2.3 
Izod Impact Strength180/1A23℃, NotchedKJ/m260 
-30℃, NotchedKJ/m215 
Charpy Impact Strength179 23℃, NotchedKJ/m260 
-30℃, NotchedKJ/m215 
Vicat Softening Temp.306 50℃/hr;1KG150 
50℃/hr;5KG145 
Heat Distortion Temp.75/A1.8MPa, unannealed125 
1.8MPa, annealed140 
Dielectric ConstantIEC 602501MHz
Volume ResistivityIEC 60093Ohm X m3.6E+14
Surface ResistivityIEC 60093Ohm9.3E+14
Coefficient of Linear Thermal Expansion11359 6.7*10-5
FlammabilityUL-941.0mm V-0
2.0mm 5VB
3.0mm 5VA
Mold Shrinkage294-4%0.4~0.6
Symbol1043 >PC<
January 12, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test

WONDERLITE® PC-6600 J01 UL Product iQ

WONDERLITE® PC-6600(Y)(a) | UL Product iQ
File Number: E56070Yellow Card™Polycarbonate (PC) “WONDERLITE”, furnished as pellets
(Y) – Optional suffix; may be suffixed with one or two alphabet but except H, unconcerned with formula or constituent changed.
(a) – Ball pressure temperature is in accordance with IEC 60695-10-2 Method B.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.0 mm, Color: ALLV-0
1.5 mm, Color: ALLV-0
2.0 mm, Color: ALL5VB, V-0
2.5 mm, Color: ALL5VA, V-0
3.0 mm, Color: ALL5VA, V-0
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.0 mm, Color: ALLV-0
1.5 mm, Color: ALLV-0
2.0 mm, Color: ALLV-0
2.5 mm, Color: ALLV-0
3.0 mm, Color: ALLV-0
FlammabilityIEC 60695-11-20
2.0 mm, Color: ALL5VB
2.5 mm, Color: ALL5VA
3.0 mm, Color: ALL5VA
Glow Wire Ignition Temperature (GWIT)IEC 60695-2-13
1.0 mm850   °C
1.5 mm875   °C
3.0 mm875   °C
Glow Wire Flammability Index (GWFI)IEC 60695-2-12
1.0 mm930   °C
1.5 mm960   °C
3.0 mm960   °C
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.0 mmPLC 3
1.5 mmPLC 3
2.0 mmPLC 2
2.5 mmPLC 2
3.0 mmPLC 0
High Amp Arc Ignition (HAI)UL 746A
1.0 mmPLC 1
1.5 mmPLC 1
2.0 mmPLC 0
2.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 2UL 746A
Dielectric Strength31   kV/mmASTM D149
Volume Resistivity1.0E+14   ohms·cmASTM D257/IEC 60093
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.0 mm130   °C
1.5 mm130   °C
2.0 mm130   °C
2.5 mm130   °C
3.0 mm130   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.0 mm120   °C
1.5 mm120   °C
2.0 mm120   °C
2.5 mm120   °C
3.0 mm120   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.0 mm130   °C
1.5 mm130   °C
2.0 mm130   °C
2.5 mm130   °C
3.0 mm130   °C
Ball Pressure Temperature135   °C
PHYSICAL PROPERTIESVALUETEST METHOD
Dimensional Change0.0   %ASTM D1042/ISO 2796

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top