Sabic Cycoloy MC8800 (PC/ABS) Resin
Cycoloy MC8800 is a high-heat, high-impact PC/ABS plastic resin. It delivers exceptional dimensional stability with a low CTE, making it a robust and reliable choice for demanding applications, particularly in the automotive sector.
- Character: PC/ABS, high heat, high impact, low CTE.
Key technical data
- Tensile Strength at Yield: 55 MPa
- Flexural Modulus: 2960 MPa
- Notched Izod Impact (23°C): 427 J/m
- Heat Deflection Temperature (HDT @ 0.45 MPa): 137°C
- Vicat Softening Temperature: 117°C
- Low Coefficient of Thermal Expansion (CTE): 6.66 x 10⁻⁵ /°C
- Melt Flow Rate (260°C/5.0 kg): 10 g/10 min
- Specific Gravity: 1.22
- Mold Shrinkage: 0.4 – 0.6%
Application
- Automotive Exterior Body Panels
- Automotive Bumper Fascias
- Durable Consumer Electronics Housings
- Industrial Equipment Housings
- Components Requiring High Heat Resistance
Features & Benefits

Related CYCOLOY™ PC/ABS Products
CYCOLOY™ Resin XCY620S
CYCOLOY™ Resin XCY620
CYCOLOY™ Resin XCM830
CYCOLOY™ Resin MC8800
CYCOLOY™ Resin MC8100
CYCOLOY™ Resin MC8002
CYCOLOY™ Resin MC1300
CYCOLOY™ Resin LG9000
CYCOLOY™ Resin HC1204HF
CYCOLOY™ Resin HC1104HF
CYCOLOY™ Resin CY8630
CYCOLOY™ Resin CP8320
CYCOLOY™ Resin CM8823
CYCOLOY™ Resin CM8622
CYCOLOY™ Resin C4220
CYCOLOY™ Resin C4210HF
CYCOLOY™ Resin C1200HF
Advanced Manufacturing