TAIRIPRO® K4535 PP Resin Injection Molding
TAIRIPRO K4535 PP Resin is a high-clarity, durable random copolymer polypropylene. With high fluidity, it flows smoothly for crystal-clear containers and housewares. Anti-static properties reduce dust, while chemical resistance protects against oils/cleaners. Its 49 kJ/m² impact strength and 95°C heat resistance ensure toughness. USP Class VI approved, it’s safe for medical/food uses.
- Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
- Character: High fluidity, High Clarity, Anti-static, Good resistance to chemical
Key technical data (ISO)
- Melt Flow Index: 35 g/10 min
- IZOD Impact Strength: 49 kJ/m²
- Specific Gravity: 0.9
- Tensile Strength: 30 MPa
- Heat Deflection Temp.: 95°C
- Flammability Rating: HB (UL 94)
- Certification: USP Class VI Approved

Applications
- High-Transparency Containers: Food storage, cosmetic jars, and display packaging with flawless clarity.
- Housewares: Shatter-resistant kitchenware, storage bins, and organizers requiring aesthetic durability.
- USP Class VI Medical Devices: IV components, surgical trays, and lab tools demanding biocompatibility and chemical resistance.

Tairipro® K4535 Datasheet
| Injection Molding Grade FCFC TAIRIPRO® K4535 Data Sheet | ||||
| Product Description: High fluidity, High Clarity, Anti-static, Good resistance to chemical | ||||
| Property | Unit | Test Method | Test Condition | Model K4535 |
| Melt Flow Index | g/10 min | ISO 1133 | 230℃ × 2.16kg | 35 |
| IZOD Impact Strength | kJ/m² | ISO 180 | 23℃,1/8″,Notched | 49 |
| IZOD Impact Strength | kJ/m² | ISO 180 | 23℃,4mm,Notched | 49 |
| Specific Gravity | – | ISO 1183 | 23℃/23℃ | 0.9 |
| Tensile Strength | Mpa | ISO 527 | 23℃,50mm/min | 30 |
| Tensile Elongation at break | % | ISO 527 | 23℃,50mm/min | >200 |
| Flexural Modulus | Mpa | ISO 178 | 23℃ | 1127 |
| Rockwell Hardness | R-scale | ISO 2039-2 | 23℃ | R-95 |
| Heat Deflection Temperature | ℃ | ISO 75/A | Unannealed,0.455Mpa 1/4″厚,120℃/h | 95 |
| Molding Shrinkage | % | FCFC Method | 23℃ | 1.5 ~ 2 |
| Combustibility | UL-94 | File No. E162823 | HB 1.5 ~ 1.65 mm | |
| All tests were run under laboratory conditions, ASTM, ISO testing procedures. | ||||
| The data are intended as a general guide only. | ||||
| Formosa Chemicals & Fibre Corp. Plastics Div. | ||||
Tairipro® K4535 UL Product iQ
| TAIRIPRO® K4535 UL Product iQ | ||
| File Number: E162823 | Polypropylene (PP), pellets | |
| Flammability | Value | Test Method |
| Flame Rating | ||
| 1.5 to 1.7 mm, ALL | HB | UL 94 |
| 1.5 to 1.7 mm, ALL | HB75 | IEC 60695-11-10, -20 |
| Electrical | Value | Test Method |
| Hot-wire Ignition (HWI) (1.5 to 1.7 mm) | PLC 3 | UL 746 |
| High Amp Arc Ignition (HAI) (1.5 to 1.7 mm) | PLC 1 | UL 746 |
| Comparative Tracking Index (CTI) | PLC 0 | UL 746 |
| High Voltage Arc Tracking Rate (HVTR) | PLC 0 | UL 746 |
| Arc Resistance | PLC 4 | ASTM D495 |
| Thermal | Value | Test Method |
| RTI Elec (1.5 to 1.7 mm) | 65.0°C | UL 746 |
| RTI Imp (1.5 to 1.7 mm) | 65.0°C | UL 746 |
| RTI Str (1.5 to 1.7 mm) | 65.0°C | UL 746 |
Related Tairipro® PP Plastics
FCFC Formosa TAIRIPRO® B8001
FCFC TAIRIPRO® F1611 PP Resin
FCFC Formosa TAIRIPRO® K9017
FCFC TAIRIPRO® S1005 PP Resin
FCFC Formosa TAIRIPRO® K8050
FCFC Formosa TAIRIPRO® K9030
FCFC Formosa TAIRIPRO® KP03B
FCFC TAIRIPRO® K1023 PP Resin
FCFC Formosa TAIRIPRO® K8025
FCFC Formosa TAIRIPRO® K8095
FCFC TAIRIPRO® S1803 PP Resin
FCFC Formosa TAIRIPRO® K8003AN
FCFC Formosa TAIRIPRO® K3029
FCFC Formosa TAIRIPRO® T3002
FCFC TAIRIPRO® F2011 PP Resin
FCFC TAIRIPRO® S1019 PP Resin
Advanced Manufacturing