LG Chem ABS AF365

LG Chem ABS Resin

LG ABS AF365 Flame Retardant Grade

LG ABS AF365 is a flame-retardant ABS resin engineered for injection molding, achieving a superior UL94 V-0 rating at just 2.0mm thickness. It combines excellent safety with high mechanical strength for critical applications.

  • Character: Flame Retardancy V-0 at 2.0mm
  • Application: Batter Case, PCB Case, Electrical/Electronic Products
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Flame Retardancy (UL94): V-1 @ 1.7mm; V-0 @ 2.0mm; 5VA @ 2.5mm
  • Comparative Tracking Index (CTI): PLC 2
  • High Amp Arc Ignition (HAI): PLC 1-2
  • Volume Resistivity: 1.0E+14 ohm·cm
  • Relative Thermal Index (RTI Elec): 85°C @ 1.8mm
  • Heat Deflection Temperature (HDT): 86°C @ 1.82 MPa
  • Tensile Strength: 46 MPa
  • Flexural Strength: 77 MPa
  • Izod Impact (Notched): 230 J/m @ 3.2mm
  • Processing Drying: 70-80°C for 3-4 hours
  • Processing Melt Temperature: 200-240°C
  • Processing Mold Temperature: 40-80°C

Application

  • Blood Pressure Monitors
  • Oxygen Concentrators
  • Pulse Monitors

Features & Benefits

Superior Flame Retardancy & Safety

LG Chem’s ABS AF365 achieves a UL94 V-0 rating at 2.0mm, ensuring enhanced fire safety for sensitive electronic components and protecting end-users from fire risks.

Excellent Mechanical & Impact Strength

This ABS resin offers high tensile strength and good impact resistance, resulting in durable, reliable components that withstand physical stress and have a longer product lifecycle.

RoHS & Regulatory Compliance

The material is fully compliant with RoHS and REACH directives, facilitating smooth global market access and meeting stringent international environmental and safety standards.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top