LG Chem ABS FR500H

LG Chem ABS Resin

LG ABS FR500H Flame Retardant Grade

LG ABS FR500H is a high-performance, flame-retardant ABS resin designed for injection molding. It achieves a superior UL94 V-0 rating at just 2.5mm thickness, making it an ideal and reliable choice for enhancing safety in sensitive electrical and electronic components.

  • Character: Flame Retardancy
  • Application: Electrical/Electronic Products
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Flammability Rating (UL94): V-0 @ 2.5mm
  • Melt Flow Index (220°C/10.0 kg): 42 g/10 min
  • Tensile Strength at Yield: 41 MPa
  • Flexural Strength: 69 MPa
  • Flexural Modulus: 2300 MPa
  • Izod Impact Strength (Notched): 22 J/m
  • Heat Deflection Temperature (HDT @ 1.82 MPa): 76 °C
  • Specific Gravity: 1.15 – 1.17
  • Fully RoHS Compliance

Application

  • Power adapters and chargers
  • Consumer electronics housings
  • Office automation equipment
  • Electrical connectors and sockets
  • Control panels and components

Features & Benefits

Superior Flame Retardant Performance

This LG Chem ABS FR500H resin delivers a critical UL94 V-0 rating at 2.5mm, significantly reducing fire propagation risks in electronic devices and ensuring compliance with stringent international safety standards.

Excellent Mechanical Strength

It offers a robust balance of tensile strength and impact resistance, providing the structural integrity needed for durable housings, brackets, and components that must withstand everyday use and assembly stresses.

High Flow for Easy Processing

With its high melt flow index, this material fills complex molds effortlessly, increasing production efficiency, reducing cycle times, and minimizing defects for superior surface quality on thin-walled parts.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top