SABIC® PC Resin PC1800

SABIC® PC Resin

Sabic PC Resin PC1800 General Purpose Grade

Sabic PC1800 is a medium-high flow, heat-stabilized polycarbonate. It’s engineered for custom compounding, offering excellent processability and robust mechanical properties for demanding industrial applications.

  • Character: medium-high flow (MFR = 10 at 300°C/1.2kg), heat stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 63 MPa
  • Flexural Modulus: 2300 MPa
  • Notched Izod Impact (23°C): 700 J/m (ASTM)
  • Heat Deflection Temp (HDT) @ 1.82 MPa: 124 °C
  • Vicat Softening Temperature: 141 °C
  • Melt Flow Rate (300°C/1.2kg): 18 g/10 min
  • Specific Gravity: 1.20
  • UL 94 Flame Rating: V-2 @ 1.6mm
  • Volume Resistivity: >1E+15 Ω·cm
  • Melt Temperature: 280 – 300 °C
  • Mold Temperature: 80 – 100 °C
  • Drying: 2-4 hours at 120°C

Application

  • Custom Compounded Materials
  • Electrical Enclosures and Housings
  • Automotive Interior Components
  • Consumer Electronics Parts
  • Industrial Machine Components
  • Connectors and Electrical Components

Features & Benefits

Excellent Melt Flow for Efficiency

With a high melt flow rate, Sabic PC1800 raw material fills complex molds easily, reducing cycle times and increasing production output for intricate parts.

Outstanding Impact Resistance & Toughness

This SABIC PC1800 plastics delivers exceptional notched Izod impact strength, ensuring your products can withstand rough handling and accidental drops without cracking.

Reliable Performance Under Heat

Its high Heat Deflection Temperature means components made from Sabic PC1800 maintain their shape and integrity in elevated temperature environments.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top