Chimei Polylac® PA-777D ABS

Chimei Polylac ABS Resin PA-777D

Polylac® PA-777D High Heat Moderate Impact ABS

POLYLAC PA-777D is an ABS resin designed for high-heat environments. It keeps its shape even at 117°C (under heavy load) and stays tough in both hot and freezing conditions. Its moderate impact strength means it won’t crack under pressure. PA-777D delivers heat resistance, durability, and ease of molding. It’s the go-to ABS resin for manufacturers who need materials that work as hard as their products do.

  • Manufacturer: CHIMEI
  • Application: Shells for heat producing household appliances, hair dryer tubes, iron casings, heaters, auto parts, water tank covers
  • Character: Ultra-high heat resistance, moderate impact strength
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Vicat Softening Temp: 124°C (1KG load)
  • Heat Distortion Temp (HDT): 117°C (annealed, 1.8MPa)
  • Tensile Strength: 45 MPa | Flexural Strength: 73 MPa
  • Izod Impact (23°C): 13 KJ/m² | Charpy Impact (23°C): 14 KJ/m²
  • Mold Shrinkage: 0.3–0.6%
  • Flammability Rating: HB (UL 94, 1.5mm thickness)

Withstands Extreme Heat Conditions

Polylac PA-777D handles up to 117°C under heavy loads and 124°C softening points. Perfect for appliances and auto parts exposed to constant heat without warping or losing shape.

Balanced Strength and Durability

It offers 45 MPa tensile strength and 13 KJ/m² impact resistance at room temperature. Tough enough for daily stress, yet flexible to avoid cracks in cold (-30°C) environments.

Safe, Easy-to-Mold Material

UL94 HB flammability rating ensures safety for household use. Low 0.3–0.6% mold shrinkage simplifies production, creating precise parts for heaters, hairdryers, and automotive components.

Chimei Polylac® PA-777D

Applications

  • Household Appliances: Hair dryer tubes, iron casings, heater components.
  • Automotive: Engine bay covers, interior trim, water tank lids.
  • Durable Electronics: Power tool housings, heat-resistant connectors.
Chimei Polylac® PA-777D Application

Polylac® PA-777D Datasheet

High Heat ABS POLYLAC® PA-777D
Product Description: Super high heat
PropertiesISO Test MethodTest ConditionUnitPA-777D
Melt Flow Index1133220℃×10KGml/10 min5.5
Mass Density118323  ℃g/cm31.06
Tensile Strength52750 mm/min, yieldMPa45
50 mm/min, breakMPa33
Tensile Elongation52750 mm/min%30
Flexural Strength1782 mm/minMPa73
Flexural Modulus1782 mm/minGPa2.3
Izod Impact Strength180/1A23℃, NotchedKJ/m213
-30℃, NotchedKJ/m27
Charpy Impact Strength17923℃, NotchedKJ/m214
-30℃, NotchedKJ/m27
Vicat Softening Temp.30650℃/hr;1KG124
50℃/hr;5KG117
Heat Distortion Temp.75/A1.8MPa, unannealed97
1.8MPa, annealed117
Coefficient of Linear Thermal Expansion113598.3 x 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.3~0.6
Symbol1043>ABS<
March 11, 2024

Polylac® PA-777D UL Product iQ

POLYLAC® PA-777D UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
Flammability (1.5 to 1.7 mm, Color: ALL)HBANSI/UL 94
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
Flammability (1.5 to 1.7 mm, Color: ALL)HB75IEC 60695-11-10
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI) (1.5 to 1.7 mm)PLC 4UL 746A
High Amp Arc Ignition (HAI) (1.5 to 1.7 mm)PLC 0UL 746A
Comparative Tracking Index (CTI)PLC 1UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 0
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical Strength (1.5 to 1.7 mm)50   °CUL 746B
Relative Thermal Index – Mechanical Impact (1.5 to 1.7 mm)50   °CUL 746B
Relative Thermal Index – Mechanical Strength (1.5 to 1.7 mm)50   °CUL 746B

Related Polylac® ABS Plastics

1 2

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top