Chimei POLYLAC PA-707 ABS Resin

Polylac® PA-707 ABS Resin General Purpose Grade


Chimei POLYLAC PA-707 is a premium General ABS resin designed for high-gloss finishes, ultra-rigid performance, and exceptional durability. Ideal for demanding industrial applications, this POLYLAC ABS grade combines aesthetics with structural integrity, making it a cost-effective choice for components requiring polished surfaces and reliable strength.

  • Character: High gloss, ultra-high rigidity, especially good tensile strength
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Melt Flow Index: 20 ml/10 min (220°C/10KG)
  • Tensile Strength: 50 MPa (yield)
  • Flexural Strength: 79 MPa
  • Heat Resistance: HDT 98°C (annealed)
  • Impact Resistance: 13 kJ/m² (23°C, notched)
  • Flammability: UL94 HB (1.5mm)
  • Mold Shrinkage: 0.4–0.7%

High-Gloss, Scratch-Resistant Finish

POLYLAC PA-707’s mirror-like surface eliminates secondary painting, saving time and costs. Perfect for consumer-facing products like telephone casings or appliance buttons where aesthetics matter.

Ultra-Rigid & Dimensional Stability

With flexural strength of 79 MPa and low mold shrinkage (0.4–0.7%), this resin resists warping, ensuring precision in parts like clock casings or office supplies that require tight tolerances.

Heat & Impact Resilience

Survives harsh conditions: Vicat softening at 104°C and HDT up to 98°C for heat resistance, plus 13 kJ/m² impact strength at 23°C. Ideal for lamp seats near bulbs or toys subjected to rough handling.

Chimei POLYLAC PA-707 ABS

Applications

  • Telephone Casings
  • Lamp Seats
  • Toys
  • Office Supplies
  • Clock Casings
  • Appliance Buttons
Chimei POLYLAC PA-707 application

Polylac® PA-707 Datasheet

General ABS POLYLAC®  PA-707
Product Description: High gloss, High rigid
PropertiesISO Test MethodTest ConditionUnitPA-707
Melt Flow Index1133 220℃×10KGml/10 min20 
Mass Density1183 23 ℃g/cm31.06 
Tensile Strength527 50 mm/min, yieldMPa50 
50 mm/min, breakMPa36 
Tensile Elongation527 50 mm/min%40 
Flexural Strength178 2 mm/minMPa79 
Flexural Modulus2 mm/minGPa2.3 
Izod Impact Strength180/1A23℃, NotchedKJ/m213 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m214 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG104 
50℃/hr;5KG99 
Heat Distortion Temp.75/A1.8MPa, unannealed83 
1.8MPa, annealed98 
Coefficient of Linear Thermal Expansion11359 8.4 x 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.7
Symbol1043 >ABS<
March  12, 2025
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

Polylac® PA-707 UL Product iQ

POLYLAC® PA-707(+) | UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
(+) – Indicate 0~0.5% acid scavengers.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
3.0 mmPLC 4
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 1UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 2
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C

Related Polylac® ABS Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top