Polylac® PA-763H Flame Retardant Grade Light Resistance
POLYLAC® PA-763H is a flame-retardant ABS resin engineered for high-flow molding, heat resistance (up to 102°C Vicat), and superior light stability. Certified for 1.5mm V-0, 5VB, and 2.5mm 5VA flammability (non-TBBA), it’s ideal for demanding applications in electronics, automotive, and appliances.
- Character: F.R. Weather resistant, High-flowability, Light-resistance, heat-resistance,1.5mm V-0,1.5mm 5VB,2.5mm 5VA (Non-TBBA series)
Key technical data (ISO)
- Flowability: Melt Flow Index = 47 ml/10 min (220°C/10kg)
- Density: 1.19 g/cm³
- Mechanical Strength: Tensile Strength = 40 MPa | Flexural Strength = 60 MPa
- Impact Resistance: Izod Impact = 17 KJ/m² (23°C)
- Heat Resistance: Vicat Softening Temp = 102°C | HDT = 92°C (annealed)
- Flame Retardancy: UL 94 1.5mm V-0, 5VB; 2.5mm 5VA
- Mold Shrinkage: 0.3–0.6%

Applications
- Electronics: Displays, modems, power panels, DVD players, remote controls.
- Automotive: Car batteries, audio consoles, rearview mirror housings.
- Office Equipment: Printer casings, fax machines, projectors, cash registers.
- Appliances: Coffee machines, power outlets, front/rear TV frames.
- Industrial: Machine boxes, large-scale multifunctional peripherals.

Polylac® PA-763H Datasheet
| Flame Retardant ABS POLYLAC® PA-763H Product Description: F.R. High flow,High heat,Weather resistant | ||||
| Properties | ISO Test Method | Test Condition | Unit | PA-763H |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 47 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.19 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 40 |
| 50 mm/min, break | MPa | 29 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 13 |
| Flexural Strength | 178 | 2 mm/min | MPa | 60 |
| Flexural Modulus | 2 mm/min | GPa | 2.1 | |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 17 |
| -30℃, Notched | KJ/m2 | 8 | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 17 |
| -30℃, Notched | KJ/m2 | 8 | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 102 |
| 50℃/hr;5KG | ℃ | 89 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 75 |
| 1.8MPa, annealed | ℃ | 92 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 8.45 x 10-5 |
| Flammability | – | UL-94 | – | 1.5mm V-0 1.5mm 5VB 2.5mm 5VA |
| Mold Shrinkage | 294-4 | – | % | 0.3~0.6 |
| Symbol | 1043 | – | – | >ABS-FR(17)< |
| March 12, 2025 Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test | ||||
Polylac® PA-763H UL Product iQ
| POLYLAC® PA-763H | UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets |
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | 5VB, V-0 | |
| 2.5 mm, Color: ALL | 5VA, V-0 | |
| 3.0 mm, Color: ALL | 5VA, V-0 | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | V-0 | |
| 2.5 mm, Color: ALL | V-0 | |
| 3.0 mm, Color: ALL | V-0 | |
| Flammability | IEC 60695-11-20 | |
| 1.5 mm, Color: ALL | 5VB | |
| 2.5 mm, Color: ALL | 5VA | |
| 3.0 mm, Color: ALL | 5VA | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 4 | |
| 2.5 mm | PLC 2 | |
| 3.0 mm | PLC 2 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 2 | |
| 2.5 mm | PLC 2 | |
| 3.0 mm | PLC 2 | |
| Comparative Tracking Index (CTI) | PLC 2 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 4 | |
| Volume Resistivity | 1.0E+14 ohms·cm | ASTM D257/IEC 60093 |
| High Voltage, Low Current Arc Resistance | PLC 5 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 2.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 60 °C | |
| 2.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 2.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
Related Polylac® ABS Plastics
Chimei Polylac® PA-763AH ABS
Chimei Polylac® PA-763H ABS
Chimei Polylac® PA-764B
Chimei Polylac® PA-764G
Chimei Polylac® PA-797 ABS
Chimei Polylac® PA-757G J08 ABS
Chimei Polylac® PA-757 J01 ABS
Chimei Polylac® PA-757 A01 ABS
Chimei Polylac® PA-756S ABS
Chimei Polylac® PA-756H ABS
Chimei Polylac® PA-747S A01 ABS
Chimei Polylac® PA-747S ABS
Chimei Polylac® PA-747R ABS
Chimei Polylac® PA-747H ABS
Chimei Polylac® PA-747F ABS
Chimei Polylac® PA-746M ABS
Chimei Polylac® PA-746H ABS
Chimei Polylac® PA-737 A03 ABS
Chimei Polylac® PA-726M ABS
Chimei Polylac® PA-717C ABS
Chimei POLYLAC® PA-709P ABS
Chimei Polylac® PA-707 ABS
Chimei Polylac® PA-77NB ABS
Chimei Polylac® PA-757H ABS
Chimei Polylac® PA-737 ABS
Chimei Polylac® PA-777E ABS
Chimei Polylac® PA-777D ABS
Chimei Polylac® PA-777B ABS
Chimei Polylac® PA-765B ABS
Chimei Polylac® PA-765A ABS
Advanced Manufacturing