Covestro Bayblend® FR630 GR

Covestro Bayblend PC ABS blend

Bayblend® FR630 GR PC/ABS Resin

Bayblend FR630 GR is a flame-retardant PC+ABS blend engineered for high-performance applications. With UL 94 V-0 certification at 1.5mm, Vicat softening at 108°C, and CQ mechanical recycled content, it delivers safety, thermal stability, and eco-efficiency for demanding industrial components. 

  • Character: (PC+ABS) blend; flame retardant; Vicat/B 120 temperature = 108 °C; UL recognition 94 V-0 at 1.5 mm
  • Application: Injection molding; Housing; Information technology
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flame Safety: UL 94 V-0 (1.5mm), 5VA (3.0mm)
  • Vicat Softening (B120): 108°C
  • HDT @1.8 MPa: 85°C
  • Tensile Modulus: 2,600 MPa
  • Notched Impact (23°C): 35 kJ/m²
  • CTI: 300 V (IEC 60112)
  • Volume Resistivity: 1E14 Ω·m
  • Water Absorption: 0.2% (equilibrium)
  • Density: 1.18 g/cm³
  • Processing Melt Temp: 240–270°C
  • Processing Drying: 4hr @80°C (max 0.02% moisture)

Application

  • Injection-Molded IT Housings: Server enclosures, laptop chassis, and router casings.
  • Fire-Safe Components: Electrical connectors, power tool housings, and control panels.
  • Industrial Equipment: Automotive electronics, HVAC systems, and consumer appliance parts.

Features & Benefits

Robust Flame Retardancy

Bayblend® FR630 GR achieves UL 94 V-0 (1.5mm) and 5VA (3.0mm) ratings, ensuring critical fire safety in electronics enclosures without compromising structural integrity. Benefit: Reduces compliance risks in high-risk environments.

Exceptional Impact & Thermal Resilience

It features 35 kJ/m² notched impact strength (23°C) and 108°C Vicat softening temperature. Benefit: Withstands drops, vibrations, and heat in IT housings, extending product lifespans.

Precision Molding Efficiency

Optimized melt flow (20 cm³/10min) and low shrinkage (0.5–0.7%) enable stable, high-yield injection molding. Benefit: Cuts production waste and costs for complex parts like thin-wall components.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top