Covestro Bayblend® FR3010 HF

Covestro Bayblend PC ABS blend

Bayblend® FR3010 HF PC/ABS Resin

Bayblend FR3010 HF is a flame-retardant, easy-flow PC+ABS blend. It offers a high UL 94 V-0 rating at just 1.5mm, excellent processability, and good impact strength, making it a reliable and efficient material for protective electronic components.

  • Character: (PC+ABS) blend; flame retardant; easy flowing; Vicat/B 120 temperature = 108 °C; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm; optimized processability; good light stability
  • Application: Injection molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flame Rating (UL 94): V-0 @ 1.5 mm thickness (5VA @ 3.0 mm)
  • Melt Flow Rate (240°C/5 kg): 25 cm³/10 min
  • Tensile Modulus: 2600 MPa
  • Notched Izod Impact (23°C): 35 kJ/m²
  • Heat Deflection Temp (HDT B @ 1.8 MPa): 90 °C
  • Relative Density: 1.18 g/cm³
  • Volume Resistivity: 1E14 Ohm·m

Application

  • Electrical Enclosures and Housings
  • Connectors and Sockets
  • Circuit Breaker Components
  • Power Distribution Units (PDUs)
  • Consumer Electronics Housings
  • Automotive Interior Electronics Components
  • Charger and Adapter Housings

Features & Benefits

Superior Flame Retardancy & Safety

It achieves a UL 94 V-0 rating at a thin 1.5mm, allowing for lighter, thinner, and safer designs in electronics and enclosures without compromising on critical safety standards.

Excellent Flow for Complex Parts

Its high melt flow rate ensures easy filling of intricate and detailed molds. This reduces injection pressure, minimizes internal stress, and boosts production efficiency for complex geometries.

High Impact Strength & Durability

It provides robust mechanical properties, including high notched impact strength. This ensures finished parts can withstand physical shocks and rough handling during assembly and throughout their service life.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top