Covestro Bayblend® FR3210 TV

Covestro Bayblend PC ABS blend

Bayblend® FR3210 TV PC/ABS Resin

Bayblend® FR3210 TV is a flame-retardant PC+ABS blend offering excellent flow, a high Vicat softening temperature of 93°C, and superior surface quality, certified UL 94 V-0 at just 1.2 mm.

  • Character: (PC+ABS) blend; flame retardant; easy flowing; Vicat/B 120 temperature = 93 °C; improved surface quality; UL recognition 94 V-0 at 1.2 mm
  • Application: Injection molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flammability Rating: UL 94 V-0 @ 1.2 mm & 1.5 mm
  • Melt Volume-Flow Rate (240°C/5 kg): 38 cm³/10 min
  • Tensile Modulus: 2700 MPa
  • Izod Notched Impact Strength (23°C): 30 kJ/m²
  • Heat Deflection Temperature (HDT B @ 0.45 MPa): 85 °C
  • Vicat Softening Temperature (B120): 93 °C
  • Density: 1180 kg/m³
  • Molding Shrinkage: 0.5 – 0.7%
  • Melt Temperature: 240 – 270 °C
  • Mold Temperature: 60 – 80 °C
  • Drying: 4 hours at 80°C (< 0.02% moisture content)

Application

  • Electrical enclosures and housings
  • Connectors and sockets
  • Consumer electronics components
  • Charger housings
  • Automotive interior components

Features & Benefits

Superior Flame Retardancy & Safety

This material achieves a UL 94 V-0 rating at a thin 1.2 mm, enabling the design of safer, lighter, and more compact components for electronics and enclosures without compromising safety.

Excellent Flow for Complex Parts

With its high melt flow rate, it fills intricate molds easily, reducing injection pressure and cycle times. This means higher productivity and fewer rejects for complex, thin-walled designs.

Enhanced Heat Resistance & Stability

A Vicat softening temperature of 93°C ensures dimensional stability and performance in elevated temperature environments, ideal for components near heat sources in electronic devices.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top