Covestro Bayblend® FR3040 W RE

Covestro Bayblend PC ABS blend

Bayblend® FR3040 W RE PC/ABS Resin

Bayblend FR3040 W RE is a flame-retardant, impact-modified PC+ABS blend. This partially bio-circular grade offers high performance and sustainability via a mass balance approach, ideal for demanding thin-wall applications.

  • Character: (PC+ABS) blend; impact modified; flame retardant
  • Application: Injection molding; Notebooks and thin-wall applications
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flame Rating: UL 94 V-0 (0.75 mm & 0.8 mm)
  • Tensile Modulus: 2650 MPa
  • Flexural Strength: 94 MPa
  • Izod Notched Impact (23°C): 48 kJ/m²
  • Heat Deflection Temp (HDT/A @ 1.8 MPa): 87 °C
  • Vicat Softening Temperature (B50): 101 °C
  • Volume Resistivity: 1E15 Ω·m
  • Melt Temperature: 250 – 280 °C
  • Mold Temperature: 60 – 80 °C
  • Moisture Content Max. Before Processing: 0.02% (Drying essential)
  • Sustainability: ISCC PLUS Mass Balance certified, partially bio-circular

Application

  • Injection Molding of complex and thin-walled components.
  • Notebooks and laptop housings, internal brackets, and components.
  • Other thin-wall applications in consumer electronics.

Features & Benefits

Superior Flame Retardancy & Safety

It achieves a UL94 V-0 rating at 0.75mm, ensuring critical fire safety for electronics enclosures and components, potentially reducing the need for additional fire shields.

Exceptional Impact Strength & Durability

It offers high notched impact strength (48 kJ/m² at 23°C), providing excellent toughness and resistance to drops and impacts in demanding use environments.

Attributed Renewable Content & Sustainability

This ISCC PLUS certified mass balance grade incorporates attributed renewable raw materials, helping you meet corporate sustainability goals without compromising on performance.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity