LG ABS HI130 General Grade
LG ABS HI130 is a high-impact, injection molding grade resin from LG Chem. It is engineered to deliver exceptional durability and a bright white color, making it ideal for demanding applications like motorcycle interiors and refrigerator components.
- Character: for injection molding, designed to have very high impact strength and bright white color
- Application: Motorcycle Interior Parts Refrigerator
Key technical data (ASTM)
- Melt Flow Index (220°C/10.0 kg): 14 g/10min
- Tensile Strength at Yield: 41 MPa
- Flexural Modulus: 1,900 MPa
- Izod Impact (Notched): 380 J/m
- Heat Deflection Temp (HDT): 85 °C @ 1.82 MPa
- Specific Gravity: 1.03
Application
- Motorcycle Interior Parts: Durable components that can withstand vibration and impact.
- Refrigerator Liners & Components: Provides structural strength and a bright, clean aesthetic.
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR630
LG Chem ABS XR474
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
Advanced Raw Material Manufacturing