LG ABS HP100S General Grade
LG ABS HP100S is a high-impact, high-whiteness ABS resin from LG Chem, ideal for injection molding and extrusion. It offers excellent stiffness, opacity, and surface finish for demanding applications.
- Character: Opaqueness, Hot Stamping, Paintability, Multi-axial Impact Strength, High Stiffness, High Impact Strength
- Application: Bags, fans, electric toothbrushes
Key technical data (ASTM)
- Tensile Strength (Yield): 40 MPa
- Flexural Modulus: 1950 MPa
- Izod Impact Strength (Notched): 43 J/m
- Rockwell Hardness (R-Scale): 95
- Heat Deflection Temperature (HDT) @ 1.82 MPa: 82 °C
- Specific Gravity: 1.05 g/cm³
- Form: Solid Pellets
Application
- Travel and cosmetic bags, cases, and housings.
- Domestic and industrial fan blades and grilles.
- Electric toothbrushes and personal care appliance housings.
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR630
LG Chem ABS XR474
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
Advanced Raw Material Manufacturing