LG ABS HP181 General Grade
LG ABS HP181 is a high-flow, general-purpose ABS resin from LG Chem, designed for injection molding. It offers excellent impact strength, dimensional stability, and superb surface quality for painting and hot stamping, making it ideal for high-volume appliance manufacturing.
- Character: Opaqueness, Hot Stamping, Paintability, Bright White, Colorability, Dimensional Stability, High Flow.
- Application: Washing machines, air conditioners, air purifiers, sweeping robots.
Key technical data (ASTM)
- Melt Flow Index (220°C/10 kg): 42 g/10min
- Tensile Strength at Yield: 42 MPa
- Flexural Modulus: 2290 MPa
- Izod Impact Strength (Notched): 26 J/m
- Heat Deflection Temperature (HDT @ 1.82 MPa): 80 °C
- Specific Gravity: 1.04 g/cm³
- Rockwell Hardness (R-Scale): 105
- Processing Moisture Content: < 0.1%
- Fully compliant with EU RoHS Directive
Application
- Washing Machine Components (Housings, Control Panels)
- Air Conditioner Grilles and Vents
- Air Purifier Housings
- Sweeping Robot Bodies and Covers
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR630
LG Chem ABS XR474
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
Advanced Raw Material Manufacturing