LG Chem ABS RS670

LG Chem ABS Resin

LG ABS RS670 Extrusion Grade

LG ABS RS670 is an extrusion-grade ABS resin engineered for superior chemical resistance to Cyclopentane foaming agents. It delivers high impact strength and excellent thermoformability, making it the ideal material for demanding applications like refrigerator liners.

  • Character: Thermoforming, Chemical Resistance to Cyclopentane, High Impact Strength.
  • Application: Refrigerator
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Tensile Strength (Yield): 49 MPa
  • Flexural Modulus: 2,500 MPa
  • Izod Impact (Notched, 23°C): 310 J/m
  • Heat Deflection Temp (1.82 MPa): 90 °C
  • Vicat Softening Temperature: 98 °C
  • Melt Flow Index (220°C/10kg): 4.5 g/10min
  • Recommended Drying: 3-4 hours at 80-90°C
  • UL Recognized Component
  • RTI (Electrical, Impakt, Strength): 60°C
  • Flammability Rating (UL 94): HB @ 0.75mm, 1.5mm, and 3.0mm

Application

  • Refrigerator and Freezer Liners
  • Interior Cabinets for Appliances
  • Components Requiring Foam-In-Place Insulation

Features & Benefits

Superior Chemical Foam Resistance

Specifically designed to withstand Cyclopentane blowing agents, it ensures long-term structural integrity in foamed insulation applications without cracking or degradation.

Exceptional Impact Strength

It maintains high toughness at both room and low temperatures, providing outstanding durability and damage resistance for finished products during handling and use.

Excellent Thermoforming Performance

It offers consistent melt flow and processing stability, allowing for deep draws and complex shapes in thermoforming processes with high production yield.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top