LG Chem ABS AF312A

LG Chem ABS Resin

LG ABS AF312A Flame Retardant Grade

LG Chem AF312A is a high-flow ABS resin with V-0 flame retardancy (1.5mm), ideal for injection molding. It offers excellent opacity, dimensional stability, and surface finish properties like paintability and hot stamping.

  • Character: fire resistance (1.5mm V-0)
  • Application: Switch panel, socket, Charge, electric control box
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Melt Flow Index: 53 g/10min (220°C, 10kg)
  • Tensile Strength: 43 MPa
  • Flexural Strength: 60 MPa
  • Flexural Modulus: 2230 MPa
  • Izod Impact Strength: 21 J/m
  • Heat Deflection Temperature: 84°C
  • Rockwell Hardness: R101
  • Flame Rating: UL94 V-0 @ 1.5mm

Application

  • Switch panels
  • Sockets
  • Chargers
  • Electric control boxes

Features & Benefits

Superior Flame Retardancy

AF312A achieves UL94 V-0 rating at just 1.5mm thickness, ensuring safety in electrical applications without compromising structural integrity.

High Flow for Easy Processing

With a melt flow index of 53 g/10min, it fills complex molds quickly, reducing cycle times and improving production efficiency for thin-walled parts.

Excellent Surface Quality

This material supports painting, hot stamping, and offers high opacity, making it perfect for aesthetically demanding components like control panels and sockets.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity