LG Chem ABS AF365B

LG Chem ABS Resin

LG ABS AF365B Flame Retardant Grade

LG ABS AF365B is a premium flame-retardant ABS resin engineered for injection molding. It achieves a critical UL 94 V-0 rating at just 2.0mm thickness, making it an ideal, reliable, and cost-effective material for demanding electrical and electronic applications.

  • Character: flammability rating of V-0 at 2.0mm
  • Application: electrical/Electronic Products, IT/OA Devices, TV, Monitor Housing
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Flammability (UL 94): V-0 @ 2.0mm | V-1 @ 1.7mm | HB @ 1.0mm
  • Melt Flow Rate (220°C/10.0 kg): 50 g/10 min
  • Tensile Strength at Yield: 39 MPa
  • Notched Izod Impact (3.2mm): 290 J/m
  • Flexural Modulus: 2250 MPa
  • Heat Deflection Temperature (1.82 MPa): 84 °C
  • Electrical: 85°C @ 1.8-3.0mm
  • Mechanical with Impact: 85°C @ 1.8-3.0mm
  • Specific Gravity: 1.16
  • Molding Shrinkage: 0.40 – 0.70%

Application

  • Electrical and Electronic Product Housings
  • IT and Office Automation (OA) Devices
  • Television (TV) Cabinets and Housings
  • Monitor Housings and Bezels

Features & Benefits

Superior Flame Retardant Performance

This material delivers a UL 94 V-0 rating at a thin 2.0mm profile. This enhances end-product safety, simplifies compliance for enclosures, and allows for more compact, modern designs without sacrificing fire safety.

Excellent Mechanical Strength

It offers a robust balance of tensile strength (39 MPa) and impact resistance (290 J/m). This ensures your housings and components are durable, can withstand assembly stresses, and resist cracking during everyday use or accidental impacts.

High Thermal Stability

With a Heat Deflection Temperature of 84°C and a high RTI, AF365B maintains its integrity when exposed to heat. This is crucial for components near heat sources, like inside TVs or monitors, preventing warping and ensuring long-term performance.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top