LG Chem ABS AF366A

LG Chem ABS Resin

LG ABS AF366A Flame Retardant Grade

LG ABS AF366A is a flame retardant ABS resin designed for injection molding, offering V-0 flammability rating at 1.5mm and excellent flow properties for high-efficiency production.

  • Character: High Flame Retardancy
  • Application: Electrical/Electronic Products, IT/OA Devices, TV, Monitor Housing.
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ASTM)

  • Flammability Rating (UL94): V-0 @ 1.5mm
  • Melt Flow Rate (220°C/10 kg): 45 g/10 min
  • Tensile Strength: 40.0 MPa
  • Notched Izod Impact (3.2mm): 310 J/m
  • Deflection Temperature (1.8 MPa): 84°C
  • Density: 1.16 g/cm³
  • Rockwell Hardness (R-scale): 98
  • Processing Method: Injection Molding
  • Drying Temperature: 80–90°C
  • Mold Temperature: 40–60°C

Application

  • Electrical and Electronic Housings
  • IT and Office Equipment Enclosures
  • TV and Monitor Bezels and Back Covers
  • Consumer Electronics Components

Features & Benefits

Superior Flame Retardancy

AF366A achieves UL94 V-0 rating at just 1.5mm, ensuring safety in high-risk electrical and electronic applications without compromising performance.

High Flow for Complex Molds

With a melt flow rate of 45 g/10min, this material fills intricate mold designs quickly, reducing cycle times and improving manufacturing efficiency.

RoHS and Compliance Ready

Fully compliant with EU RoHS directives and free from restricted substances, making it ideal for global markets and environmentally conscious brands.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine