LG ABS AF366F Flame Retardant Grade
LG ABS AF366F is a flame retardant ABS resin engineered for injection molding. It delivers a superior V-0 flammability rating at just 1.5mm thickness and features excellent high flow properties for complex, thin-walled designs.
- Character: High Flame Retardancy, High Flow
- Application: Television, Electrical/Electronic Products
Key technical data (ASTM)
- Flammability (UL 94): V-0 @ 1.5mm, 2.0mm, 2.5mm, 3.0mm
- Melt Flow Index (220°C/10 kg): 70 g/10min
- Tensile Strength (Yield): 41 MPa
- Flexural Modulus: 2450 MPa
- Izod Impact (Notched, 3.2mm): 200 J/m
- Heat Deflection Temp (1.82 MPa): 83 °C
- Specific Gravity: 1.17
- RoHS & Phthalates: Fully Compliant
Application
- Television Cabinets and Components
- Electrical and Electronic Product Housings
- Office Automation Equipment
- Consumer Appliances
- Components Requiring High Flame Safety
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR630
LG Chem ABS XR474
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
Advanced Raw Material Manufacturing