LG Chem ABS AF367H

LG Chem ABS Resin

LG ABS AF367H Flame Retardant Grade

LG Chem’s ABS AF367H is a high-performance, flame-retardant ABS resin designed for injection molding. It offers exceptional thermal stability and a V-0 fire resistance rating at 2.5mm, making it a reliable and safe choice for demanding electronic and healthcare applications.

  • Character: fire resistance (2.5mm V-0).
  • Application: Blood pressure monitor, oxygen concentrator, power supply development, socket.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Flame Retardancy (UL94): V-0 @ 2.5mm
  • Melt Flow Index (220°C/10 kg): 30 g/10min
  • Tensile Strength at Yield: 43 MPa
  • Flexural Modulus: 2300 MPa
  • Izod Impact Strength (Notched): 20 J/m
  • Heat Deflection Temperature (HDT @ 1.82 MPa): 85 °C
  • Specific Gravity: 1.15 g/cm³
  • Fully compliant with EU RoHS Directive

Application

  • Blood Pressure Monitors
  • Oxygen Concentrators
  • Power Supply Housings / Development
  • Sockets and Electrical Connectors

Features & Benefits

Superior Flame Retardant Safety

This material achieves a UL94 V-0 rating at 2.5mm, significantly enhancing end-product safety and helping you meet strict international safety standards for electronics and medical devices.

Excellent Thermal Resistance

With a Heat Deflection Temperature of 85°C, AF367H maintains structural integrity under thermal stress, ensuring reliable performance in devices that generate heat during operation.

Easy and Stable Processing

Its high melt flow rate (30 g/10min) ensures excellent fill characteristics and short cycle times during injection molding, boosting your production efficiency and reducing manufacturing costs.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity