LG ABS FR530 Flame Retardant Grade
LG ABS FR530 is a premium TBPC flame retardant ABS resin from LG Chem, engineered for injection molding. It achieves a superior UL94 V-0 rating at just 2.0mm, offering exceptional safety, thermal stability, and excellent colorability for demanding applications.
- Character: Flame Retardancy, Thermal Stability, Colorability, Imflammability
- Application: Electrical/Electronic Products Medical Equipment Housing
Key technical data (ASTM)
- Flammability Rating (UL94): V-0 @ 2.0mm
- Melt Flow Index (220°C/10.0kg): 40 g/10min
- Tensile Strength at Yield: 42 MPa
- Flexural Modulus: 2500 MPa
- Izod Impact Strength (Notched): 22 J/m
- Heat Deflection Temperature (1.82 MPa, Annealed): 84 °C
- Specific Gravity: 1.15 – 1.17
- RoHS Compliance: Fully Compliant (SGS Certified)
Application
- Electrical/Electronic Products Housing (e.g., chargers, power strips, connectors)
- Medical Equipment Housing and Components
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR630
LG Chem ABS XR474
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
Advanced Manufacturing