LG ABS TR551 Transparent Grade
LG Chem TR551 is a transparent ABS resin engineered for injection molding. It delivers an exceptional balance of high optical clarity, superior stiffness, and remarkable impact resistance for demanding technical applications.
- Character: Transparency, High Hardness, High Stiffness
- Application: Washing Machine, Refrigerator, Electrical/Electronic Products, Miscellaneous Goods
Key technical data (ASTM)
- Specific Gravity: 1.12
- Melt Flow Index (220°C/10Kg): 8 g/10min
- Tensile Strength (Yield): 59 MPa
- Flexural Modulus: 2,850 MPa
- Izod Impact (Notched, 3.2mm @ 23°C): 125 J/m
- Heat Deflection Temp (1.82MPa, Unannealed): 87 °C
- Light Transmittance (3.2mm): 90%
- Haze: 1.9%
- UL 94 Flammability Rating (1.5mm & 3.0mm): HB
- Relative Thermal Index (RTI): 50 °C
- Full RoHS & REACH compliant
Application
- Washing Machine: For see-through detergent dispensers and control panel covers.
- Refrigerator: For durable, transparent vegetable drawers, bin fronts, and interior trim.
- Electrical/Electronic Products: For protective covers, housings, and lenses requiring clarity and impact resistance.
- Miscellaneous Goods: For a variety of consumer and industrial products requiring a robust transparent plastic.
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR630
LG Chem ABS XR474
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
Advanced Manufacturing