LG Chem ABS XG571

LG Chem ABS Resin

LG ABS XG571 Transparent Grade

LG ABS XG571 is a premium transparent ABS resin engineered for injection molding. It delivers an exceptional combination of high translucency, superior surface gloss, and excellent flow characteristics for complex, high-quality components.

  • Character: Translucency, High Gloss, High Flow
  • Application: Air Conditioner, Water Purifier, Air Purifier, Electrical/Electronic Products
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Melt Flow Index (220°C, 10 kg): 51 g/10min
  • Tensile Strength at Yield: 48 MPa
  • Flexural Modulus: 2650 MPa
  • Izod Impact Strength (Notched, 3.2mm): 170 J/m
  • Heat Deflection Temperature (1.82 MPa): 87 °C
  • Specific Gravity: 1.05
  • Flammability Rating (UL 94): HB
  • Relative Thermal Index (RTI Elec): 50.0 °C
  • RoHS & Phthalates Compliance

Application

  • Air Conditioner Components (e.g., transparent lids, dials)
  • Water Purifier Housings (e.g., filter heads, window covers)
  • Air Purifier Components
  • Electrical/Electronic Product Enclosures

Features & Benefits

Superior Optical Clarity & Aesthetics

This material offers outstanding translucency and a high-gloss finish, enhancing the visual appeal and perceived value of your products without the need for painting.

Excellent Processing Efficiency

With its high flow rate, LG ABS XG571 fills intricate molds easily, reducing cycle times and improving production efficiency for complex parts with thin walls.

Reliable Mechanical Strength

It provides a robust balance of good impact resistance and structural integrity, ensuring durable and reliable performance in final applications.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity