SABIC® PC Resin PC5800

SABIC® PC Resin

Sabic PC Resin PC5800 Injection Molding Grade

Sabic PC5800 is a very high flow polycarbonate, ideal for optical media and complex, thin-walled components requiring superior clarity and process efficiency.

  • Character: very high flow (MFR = 8.9 at 250°C/1.2kg) polycarbonate
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Melt Flow Rate (250°C/1.2kg): 8.9 g/10 min
  • Light Transmission (2.54mm): >90%
  • Haze (2.54mm): <0.7%
  • Heat Deflection Temp (1.82 MPa): 122 °C
  • Izod Impact, Notched (23°C): 15 kJ/m²
  • Flexural Modulus: 2300 MPa
  • Specific Gravity: 1.2
  • Mold Shrinkage, Flow: 0.5 – 0.7%

Application

  • the optical media market

Features & Benefits

Exceptional High-Flow Molding

With a high melt flow rate, Sabic PC5800 fills intricate molds easily, reducing cycle times and improving productivity for complex part geometries.

Superior Optical Clarity

This material offers over 90% light transmission and low haze, ensuring brilliant transparency and visual appeal for applications where clarity is critical.

Outstanding Impact Resistance

PC5800 provides excellent toughness, even at low temperatures, resulting in durable and reliable parts that resist cracking and withstand physical stress.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity