Polylac® PA-765A Flame Retardant High Flow ABS Resin
POLYLAC PA-765A is a flame-retardant ABS resin. It meets strict fire standards (UL94 V-0 at 2.1mm, 5VA at 2.5mm), ideal for electronics, car parts, and appliances. Its high flow (48 ml/10min) fills complex molds smoothly, perfect for thin walls like power outlets or printer casings. Durable against impacts (22 kJ/m²) and heat (up to 93°C), it’s trusted for coffee machines, TV frames, and more. UL-certified and Yellow Card-compliant. For details, check the PA-765A datasheet.
- Manufacturer: CHIMEI
- Character: High flowability, 1.5mm V-1, 2.1mm V-0, 2.1mm 5VB, 2.5mm 5VA (TBBA series)

Download
Access essential product documentation including technical datasheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.

Polylac® PA-765A Datasheet
| Flame Retardant ABS POLYLAC® PA-765A | ||||
| Product Description: F.R. High flow | ||||
| Properties | ISO Test Method | Test Condition | Unit | PA-765A |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 48 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.17 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 39 |
| 50 mm/min, break | MPa | 29 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 10 |
| Flexural Strength | 178 | 2 mm/min | MPa | 56 |
| Flexural Modulus | 178 | 2 mm/min | GPa | 1.8 |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 22 |
| -30℃, Notched | KJ/m2 | 10 | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 23 |
| -30℃, Notched | KJ/m2 | 10 | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 93 |
| 50℃/hr;5KG | ℃ | 79 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 76 |
| 1.8MPa, annealed | ℃ | 84 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 8.48 x 10-5 |
| Flammability | – | UL-94 | – | 1.5mm V-1 |
| 2.1mm V-0 | ||||
| 2.1mm 5VB | ||||
| 2.5mm 5VA | ||||
| Mold Shrinkage | 294-4 | – | % | 0.3~0.6 |
| Symbol | 1043 | – | – | >ABS-FR(17)< |
| March 11, 2024 | ||||
Polylac® PA-765A UL Product iQ
| POLYLAC® PA-765A UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets |
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | V-1 | |
| 2.1 mm, Color: ALL | 5VB | |
| V-0 | ||
| 2.5 mm, Color: ALL | 5VA | |
| V-0 | ||
| 3.0 mm, Color: ALL | 5VA | |
| V-0 | ||
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | V-1 | |
| 2.1 mm, Color: ALL | V-0 | |
| 2.5 mm, Color: ALL | V-0 | |
| 3.0 mm, Color: ALL | V-0 | |
| Flammability | IEC 60695-11-20 | |
| 2.1 mm, Color: ALL | 5VB | |
| 2.5 mm, Color: ALL | 5VA | |
| 3.0 mm, Color: ALL | 5VA | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 2.1 mm | PLC 3 | |
| 2.5 mm | PLC 3 | |
| 3.0 mm | PLC 0 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 2.1 mm | PLC 0 | |
| 2.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| Comparative Tracking Index (CTI) | PLC 1 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 2 | |
| High Voltage, Low Current Arc Resistance | PLC 7 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 85 °C | |
| 2.1 mm | 85 °C | |
| 2.5 mm | 85 °C | |
| 3.0 mm | 85 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 80 °C | |
| 2.1 mm | 80 °C | |
| 2.5 mm | 80 °C | |
| 3.0 mm | 80 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 85 °C | |
| 2.1 mm | 85 °C | |
| 2.5 mm | 85 °C | |
| 3.0 mm | 85 °C | |
| Report Date: 1983-06-23 | ||
| 2.5 mm | 80 °C | |
| 3.0 mm | 80 °C | |
Related Polylac® ABS Plastics
Chimei Polylac® PA-726M ABS
Chimei Polylac® PA-717C ABS
Chimei POLYLAC® PA-709P ABS
Chimei Polylac® PA-707 ABS
Chimei Polylac® PA-77NB ABS
Chimei Polylac® PA-757H ABS
Chimei Polylac® PA-737 ABS
Chimei Polylac® PA-777E ABS
Chimei Polylac® PA-777D ABS
Chimei Polylac® PA-777B ABS
Chimei Polylac® PA-765B ABS
Chimei Polylac® PA-765A ABS