Covestro Bayblend® FR3030

Covestro Bayblend PC ABS blend

Bayblend® FR3030 PC/ABS Resin

Bayblend FR3030 is a flame-retardant (PC+ABS) blend engineered for high safety and process efficiency. It delivers UL 94 V-0 certification at just 1.5 mm thickness, halogen-free compliance (DIN VDE 0472), and exceptional thermal stability (Vicat 115°C). Ideal for extrusion and vacuum forming, it combines ease of processing with rigorous fire safety standards.

  • Character: (PC+ABS) blend; flame retardant; Vicat/B 120 temperature = 115°C; good extrusion and vacuum-forming behaviour; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 1.0 mm
  • Application: Extrusion
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Tensile Modulus: 2,650 MPa
  • Impact Strength (Notched, 23°C): 40 kJ/m²
  • Strain at Break: >50%
  • Vicat Softening Temp (B120): 115°C
  • HDT (0.45 MPa): 106°C
  • UL 94 Rating (1.5 mm): V-0
  • Glow Wire (GWFI, 1.0 mm): 960°C
  • CTI (Comparative Tracking Index): 350
  • Volume Resistivity: 1E15 Ω·m
  • Molding Shrinkage: 0.5–0.7%
  • Density: 1,190 kg/m³
  • Water Absorption: 0.2% (equilibrium)

Application

  • Electrical Conduits & Cable Trays
  • HVAC Ducting Systems
  • Protective Industrial Guards
  • Transportation Interior Trims
  • EV Battery Housing Components

Features & Benefits

Reliable Flame Resistance

Bayblend FR3030 (PC+ABS) blend achieves UL 94 V-0 at 1.5 mm and glow wire ignition resistance (GWFI 960°C), eliminating secondary flame treatments. Perfect for electrical enclosures in high-risk environments.

Superior Processing Flexibility

Optimized for extrusion and vacuum forming, this material ensures smooth flow (MVR 11 cm³/10min) and low shrinkage (0.5–0.7%). Reduces waste and accelerates production of complex parts like automotive ducts.

Robust Mechanical Performance

High impact strength (40 kJ/m² at 23°C) and thermal resilience (HDT 106°C @ 0.45 MPa) ensure durability under stress. Ideal for protective housings in EVs or industrial equipment.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top