LG Chem ABS AF366F

LG Chem ABS Resin

LG ABS AF366F Flame Retardant Grade

LG ABS AF366F is a flame retardant ABS resin engineered for injection molding. It delivers a superior V-0 flammability rating at just 1.5mm thickness and features excellent high flow properties for complex, thin-walled designs.

  • Character: High Flame Retardancy, High Flow
  • Application: Television, Electrical/Electronic Products
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Flammability (UL 94): V-0 @ 1.5mm, 2.0mm, 2.5mm, 3.0mm
  • Melt Flow Index (220°C/10 kg): 70 g/10min
  • Tensile Strength (Yield): 41 MPa
  • Flexural Modulus: 2450 MPa
  • Izod Impact (Notched, 3.2mm): 200 J/m
  • Heat Deflection Temp (1.82 MPa): 83 °C
  • Specific Gravity: 1.17
  • RoHS & Phthalates: Fully Compliant

Application

  • Television Cabinets and Components
  • Electrical and Electronic Product Housings
  • Office Automation Equipment
  • Consumer Appliances
  • Components Requiring High Flame Safety

Features & Benefits

Superior Thin-Wall Flame Retardancy

It achieves a UL 94 V-0 rating at 1.5mm, ensuring critical fire safety compliance for compact, modern electronic devices and enclosures.

Excellent High Flow Processing

Its high fluidity (70 g/10min) ensures easy filling of intricate molds, reducing injection pressure and minimizing internal stresses for higher production yields.

Compliant & Safe Material Composition

Fully complies with RoHS and phthalate regulations, making it a safe and reliable choice for global consumer electronics and electrical applications.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top