LG Chem ABS AF366HF

LG Chem ABS Resin

LG ABS AF366HF Flame Retardant Grade

LG Chem AF366HF is a high-flow ABS resin engineered for injection molding. It offers superior V-0 flame retardancy at 1.5mm, excellent thermal resistance, and great stability, making it ideal for demanding industrial electronics and appliance applications.

  • Character: fire resistance (1.5mm V-0).Opaqueness, High Flame Retardancy, Bright White.
  • Application: Industrial electronic control boxes, purifiers, heaters.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Flame Rating: UL94 V-0 (1.5mm thickness)
  • Tensile Strength: 42.5 MPa
  • Flexural Modulus: 2200 MPa
  • Izod Impact Strength: 20 J/m
  • Heat Deflection Temperature (HDT): 82°C @ 1.82 MPa
  • Processing Drying: 70-80°C for 3-4 hours
  • Melt Temperature: 200-230°C
  • Mold Temperature: 40-60°C
  • RoHS Directive Compliant
  • Appearance: Opaque, Bright White pellets
  • Specific Gravity: 1.15 g/cm³

Application

  • Industrial Electronic Control Boxes & Housings
  • Air & Water Purifiers
  • Heating Appliances & Heaters

Features & Benefits

Superior Flame Retardant Performance

This LG ABS AF366HF material achieves a UL94 V-0 rating at just 1.5mm thickness, ensuring critical safety compliance and protecting sensitive internal components in case of an electrical fault.

Enhanced Thermal Resistance & Stability

With a Heat Deflection Temperature of 82°C, this ABS resin maintains structural integrity when exposed to heat, preventing warping or deformation in enclosed environments like control boxes.

Excellent Processing & High Flow

Its high flow feature simplifies filling complex and thin-walled mold designs, reducing injection pressure and cycle times for increased manufacturing efficiency and lower production costs.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top