Bayblend® T70 X RE PC/ABS Resin
Covestro’s Bayblend® T70 X RE is a partially bio-circular PC+ABS blend (ISCC PLUS certified), combining sustainability with high performance. It delivers heat resistance (Vicat 124°C), low VOC emissions, excellent impact strength, and easy processing—ideal for eco-conscious industrial applications.
- Character: (PC+ABS) blend; Vicat/B 120 temperature = 124 °C; good injection molding processing behaviour (easy flowing); excellent long-term ageing behaviour under humid conditions; good painting performance; improved chemical resistance; low VOC emissions and odour
- Application: Injection molding; General purpose
Key technical data (ISO)
- Tensile Modulus: 2,250 MPa | Yield Stress: 53 MPa
- Puncture Impact (23°C): 4,300 N (force) / 48 J (energy)
- HDT @1.8 MPa: 103°C | Vicat Softening (B120): 124°C
- Linear Expansion: 0.7 x 10⁻⁴/K (low warpage)
- UL 94 Rating: HB (0.85 mm thickness)
- Water Absorption: 0.1% (equilibrium, 50% RH)
- Melt Temp: 270–290°C | Mold Temp: 70–90°C
- Drying: 4 hrs @ 95–110°C (<0.01% moisture)
Application
- Consumer Electronics: Durable housings for power tools, routers.
- Automotive Interiors: Trim components, panels.
- Industrial Enclosures: Control boxes, connectors.
- General Purpose: High-strength structural parts requiring sustainability.
Features & Benefits
Related Bayblend® PC/ABS Products
Covestro Bayblend® M850 XF
Covestro Bayblend® M850 XF RE
Covestro Bayblend® M750 RE CQ
Covestro Bayblend® M303 FR
Covestro Bayblend® FR3040 W RE
Covestro Bayblend® M750
Covestro Bayblend® FR3311 TV
Covestro Bayblend® FR3020 W BBS910
Covestro Bayblend® FR3210 TV
Covestro Bayblend® FR3200 TV
Covestro Bayblend® FR3110 TV
Covestro Bayblend® M301 FR
Covestro Bayblend® FR3040 R35
Covestro Bayblend® FR3010 HF
Covestro Bayblend® FR3008 RE
Covestro Bayblend® FR3008 HR
Covestro Bayblend® FR3006 HF
Covestro Bayblend® FR3000 HI
Advanced Manufacturing