Covestro Bayblend® FR3001

Covestro Bayblend PC ABS blend

Bayblend® FR3001 PC/ABS Resin Flame Retardant Grade

Covestro PC+ABS Bayblend® FR3001 is a flame-retardant (UL 94 V-0 at 1.5mm), non-reinforced blend engineered for high-performance applications. With a Vicat softening temperature of 103°C and excellent flow properties, it ensures safety, durability, and ease of processing for thin-walled components in demanding industries.

  • Character: (PC+ABS) blend; flame retardant; Vicat/B 120 temperature = 103 °C; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm; Flame retardant
  • Application: Injection molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Flame Resistance: UL 94 V-0 (1.5mm), 5VA (3.0mm)
  • Glow Wire (GWFI): 960°C (2.0mm)
  • Tensile Modulus: 2,700 MPa
  • Notched Impact: 15 kJ/m² (23°C)
  • Thermal HDT: 98°C (0.45 MPa)
  • Vicat Softening: 103°C
  • Electrical CTI: 600V
  • Volume Resistivity: 1E14 Ω·m
  • Processing Melt Temp: 240–270°C
  • Mold Temp: 60–90°C
  • Drying: 4h at 80°C (≤0.02% moisture)

Application

  • Electronics: Connectors, switches, and smartphone housings.
  • Automotive: Dashboard components, fuse boxes, and interior trims.
  • Industrial: Power tool casings, control panels, and enclosures.
  • Consumer Tech: Thin-walled laptop chassis and charger housings.

Features & Benefits

Superior Flame Resistance

It achieves UL 94 V-0 (1.5mm) and 5VA (3.0mm) ratings, eliminating the need for secondary flame treatments. Ideal for electronics and automotive parts requiring strict fire safety compliance.

High Impact & Thermal Stability

It boasts 15 kJ/m² notched impact strength at 23°C and heat deflection up to 98°C (0.45 MPa). Ensures durability in rugged environments, from power tools to industrial housings.

Easy Processing & Consistency

Optimized flow (480mm spiral flow) and low shrinkage (0.5–0.7%) enable complex mold filling and dimensional stability. Reduces scrap rates and shortens production cycles.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top