LG ABS AF365S is a flame retardant ABS resin engineered for extrusion and blow molding. It achieves a superior UL94 V-0 rating at just 2.0mm thickness, making it an ideal, safe, and efficient material choice for demanding applications.

  • Character: Flame Retardant V-0 at 2.0mm
  • Application: Battery Tray
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ASTM)

  • Flammability (UL94): V-0 @ 2.0mm, 2.5mm, 3.0mm | V-1 @ 1.7mm
  • Melt Flow Index (220°C/10kg): 7.5 g/10min
  • Tensile Strength at Yield: 47 MPa
  • Flexural Modulus: 2550 MPa
  • Izod Impact (Notched, 3.2mm): 290 J/m
  • Heat Deflection Temp (1.82MPa): 87 °C
  • Specific Gravity: 1.16
  • RoHS Compliance: Fully Conforms to EU Directive 2015/863

Application

  • Battery Trays for Electric Vehicles and Energy Storage Systems

Features & Benefits

Superior Flame Retardant Performance

This material is certified UL94 V-0 at 2.0mm, ensuring critical safety in components where fire resistance is a non-negotiable requirement, protecting both products and end-users.

Excellent Processing Versatility

Optimized for extrusion and blow molding processes, LG Chem AF365S offers excellent melt flow, allowing for easier and more efficient production of large, complex parts like battery housings.

Compliant and Safe Material

This ABS AF365S LG Chem resin is fully compliant with RoHS directives, ensuring your products meet strict international environmental and safety regulations without compromising on performance.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top