LG ABS EF378L Flame Retardant Grade
LG ABS EF378L is a non-halogen, flame-retardant ABS resin designed for injection molding. It achieves a critical UL 94 V-2 rating at just 0.8mm thickness, making it an ideal, safer choice for thin-walled electronic components.
- Character: Flame Retardancy, Non-Halogen
- Application: MFP (Multi-Function Printer), Sound Bar, Electrical/Electronic Products
Key technical data (ISO)
- Flame Retardancy (UL 94): V-2 @ 0.8mm, V-2 @ 3.0mm
- Relative Thermal Index (UL 746): 60°C (Elec, Imp, Str)
- Melt Flow Rate (220°C / 10kg): 55 g/10min
- Tensile Strength: 45 MPa
- Flexural Modulus: 2,600 MPa
- Izod Impact Strength (Notched): 14 kJ/m²
- Heat Deflection Temp (1.8MPa): 75 °C
- Specific Gravity: 1.06
- Regrind Compatibility: Virgin material properties maintained with up to 50% regrind content.
- Fully compliant with RoHS and REACH regulations
Application
- MFP (Multi-Function Printer) Components
- Sound Bars and Audio Equipment Housings
- Electrical and Electronic Product Enclosures
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR630
LG Chem ABS XR474
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
Advanced Raw Material Manufacturing