LG Chem ABS TR556

LG Chem ABS Resin

LG ABS TR556 Transparent Grade

LG ABS TR556 is a high-performance transparent ABS resin from LG Chem, engineered for injection molding and extrusion. It delivers an exceptional balance of optical clarity, high impact strength, and excellent chemical resistance.

  • Character: Transparency, Chemical Resistance, High Impact Strength
  • Application: Electrical/Electronic Products, Miscellaneous Goods
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Specific Gravity: 1.09
  • Melt Flow Index (220°C/10Kg): 5 g/10min
  • Tensile Strength at Yield: 49 MPa
  • Flexural Modulus: 2300 MPa
  • Izod Impact Strength (Notched, 23°C): 195 J/m
  • Heat Deflection Temp (1.82 MPa, Unannealed): 85 °C
  • Vicat Softening Temperature: 93 °C
  • Light Transmittance (3.2mm): 90%
  • Flammability Rating (UL94): HB (1.5mm & 3.0mm)
  • Relative Thermal Index (RTI): 50 °C
  • RoHS & Phthalates Compliant

Application

  • Electrical/Electronic Products: Transparent covers, meter windows, appliance components, and protective housings.
  • Miscellaneous Goods: Durable consumer products, cosmetic cases, office supplies, and high-impact transparent containers.

Features & Benefits

Superior Optical Clarity

With 90% light transmittance and low haze, TR556 produces brilliantly clear components, ideal for products where visual appeal and visibility of internal parts are critical.

Exceptional Impact Resistance

This material maintains high toughness, even at low temperatures (-30°C), ensuring durable parts that resist cracking or breaking from physical shock during use or assembly.

Strong Chemical Resistance

TR556 reliably withstands exposure to various chemicals, protecting components from degradation and preserving their appearance and structural integrity over time.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity