TAIRILAC® AC3830 PC Resin Self Extinguishing Grade
Tairilite AC3830 is a versatile polycarbonate resin produced by FCFC FORMOSA for demanding applications. This halogen-free, UV-resistant material combines exceptional light diffusion, mid-flow processability, and self-extinguishing properties (UL 94 V-0) in a single solution—ideal for optical components and safety-critical parts.
- Character: Light diffusion, Mid flow, UV resistance, Halogen free
- Application: Diffusion board, Diffusion lamp, Diffusion injection lampshade, Diffusion injection-blow bulb
Key technical data (ISO)
- Melt Flow: 12 g/10 min (300°C, 1.2 kg)
- Impact Strength: 70 kJ/m² (Charpy, notched)
- Thermal Stability: HDT 128°C (1.8 MPa)
- Flame Rating: UL 94 V-0 (1.0–3.0 mm), 5VA (3.0 mm)
- Electrical Safety: CTI PLC 2, HWI/HAI PLC 0-1
- Outdoor Durability: f1-rated (UV/water resistance)
- Processing: Pre-dry at 120°C for 4–8 hrs; max barrel temp 330°C.
Features & Benefits

Application

Related Tairilite® PC Plastics
FCFC Formosa TAIRILITE® AC2916
FCFC Formosa TAIRILITE® AC2955
FCFC Formosa TAIRILITE® AC9830
FCFC Formosa TAIRILITE® AC9144
FCFC Formosa TAIRILITE® AC9140
FCFC Formosa TAIRILITE® AC2820
FCFC Formosa TAIRILITE® AC2854
FCFC Formosa TAIRILITE® AC2856
FCFC Formosa TAIRILITE® AC3873
FCFC Formosa TAIRILITE® AC3832
FCFC Formosa TAIRILITE® AC3854
FCFC Formosa TAIRILITE® AC3853
FCFC Formosa TAIRILITE® AC3843
FCFC Formosa TAIRILITE® AC3630
FCFC Formosa TAIRILITE® AC3600-AF
FCFC Formosa TAIRILITE® AC3600
FCFC Formosa TAIRILITE® AC3900
FCFC Formosa TAIRILITE® AC3839
Advanced Manufacturing